Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0150 cm/cm | 0.00500 - 0.0150 in/in | Average value: 0.00940 cm/cm Grade Count:10 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00750 cm/cm | 0.00500 - 0.00750 in/in | Average value: 0.00650 cm/cm Grade Count:3 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00800 cm/cm | 0.00500 - 0.00800 in/in | Average value: 0.00641 cm/cm Grade Count:22 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0100 cm/cm | 0.00500 - 0.0100 in/in | Average value: 0.00727 cm/cm Grade Count:22 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00700 cm/cm | 0.00500 - 0.00700 in/in | Average value: 0.00600 cm/cm Grade Count:8 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00600 cm/cm | 0.00500 - 0.00600 in/in | Average value: 0.00550 cm/cm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0240 cm/cm | 0.00500 - 0.0240 in/in | Average value: 0.0171 cm/cm Grade Count:8 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0140 cm/cm | 0.00500 - 0.0140 in/in | Average value: 0.00930 cm/cm Grade Count:32 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.100 cm/cm | 0.00500 - 0.100 in/in | Average value: 0.0118 cm/cm Grade Count:62 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0105 cm/cm | 0.00500 - 0.0105 in/in | Average value: 0.00819 cm/cm Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0165 cm/cm | 0.00500 - 0.0165 in/in | Average value: 0.00972 cm/cm Grade Count:9 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0250 cm/cm | 0.00500 - 0.0250 in/in | Average value: 0.0145 cm/cm Grade Count:34 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0220 cm/cm | 0.00500 - 0.0220 in/in | Average value: 0.00916 cm/cm Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0170 cm/cm | 0.00500 - 0.0170 in/in | Average value: 0.0113 cm/cm Grade Count:11 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |