Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.483 - 36.2 GPa
70.0 - 5250 ksi
Average value: 4.87 GPa Grade Count:205
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Flexural Modulus 0.483 GPa
70.0 ksi
ASTM D790
Techmer ES HiFill® TPU 1000
Availability: North AmericaForms: PelletsFeatures: High DensityAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 0.483 GPa
70.0 ksi
ASTM D790
Techmer ES Luriblend® PE 5902
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc...
Flexural Modulus 0.483 GPa
70.0 ksi
ASTM D790
Techmer ES Luriblend® PE 5903
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc...
Flexural Modulus 0.483 GPa
70.0 ksi
ASTM D790
Techmer ES HiFill FR® PA6/6 GF10 FR BK 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightFeatures: Flame Retardant Appearance: BlackProcessing Method: Injection MoldingInformation provided by..