Polymer Property : Dielectric Strength = 17.3 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 17.3 kV/mm
439 kV/in
ASTM D149
Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer
Description: Durable polyamide (nylon) material for real-world physical testing and functional useFeatures: Excellent surface resolution and feature detailEasy-to-processCompliant with USP Class VI ..
Dielectric Strength 17.3 kV/mm
440 kV/in
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating
Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the..
Dielectric Strength 17.3 kV/mm
440 kV/in
Resinlab® EP1325LV Thixotropic, Heat Curing Epoxy Adhesive
Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where ..
Dielectric Strength 17.3 kV/mm
440 kV/in
Resinlab® EP1385 Clear Epoxy Formulation
Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w..
Dielectric Strength 17.3 kV/mm
439 kV/in
Short Time; ASTM D149
Plenco 50240 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Elastoblend® PA6/6 GF30 IM HS L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri..
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Elastoblend® PA6/6 GF4 IM L LE
Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant, Low Extractables and Impact ModifiedAppearance: Natural ColorInformation provided by TP Composite..
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PA6/6 GF33 BK024 33% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp..
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Plastiblend® PA6/6,6 109 L Nylon 6/66
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Copolymer and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Plastiblend® PA6/6,6 IM HS L Nylon 6/66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold..
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Elastoblend® PA6/6 IM 3757 HS L Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Fast Molding Cycle, High Flow, Heat Stabilized, Lubricant and Impact ModifiedProcessing Met..
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL Fil..
Dielectric Strength >= 17.3 kV/mm

@Thickness 3.17 mm
>= 440 kV/in

@Thickness 0.125 in
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive
Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e..
Dielectric Strength 17.3 kV/mm

@Thickness 3.17 mm
440 kV/in

@Thickness 0.125 in
Master Bond EP21ARHT Two component epoxy adhesive, sealant, coating and encapsulating system
Product Description: Master Bond EP21ARHT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a convenient 100 to 50 mix ratio by weight an..
Dielectric Strength 17.3 kV/mm

@Thickness 3.17 mm
440 kV/in

@Thickness 0.125 in
Master Bond EP21ARHTND Two component epoxy adhesive, sealant, coating and encapsulating system
Product Description: Master Bond EP21ARHTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a convenient 100 to 50 mix ratio by weight and is formulat..
Dielectric Strength 17.3 kV/mm

@Thickness 3.17 mm
440 kV/in

@Thickness 0.125 in
Master Bond EP21LV-LO Two Component, Lower Viscosity, Room Temperature Curing Epoxy System
Product Description: Master Bond EP21LV-LO is a two component, lower viscosity, room temperature curing epoxy system for high performance bonding, sealing, coating and encapsulation. This user frien..
Dielectric Strength 17.3 kV/mm

@Thickness 3.17 mm
440 kV/in

@Thickness 0.125 in
Master Bond EP41S-1HT Solvent Resistant Adhesive, Sealant and Coating
Description: Master Bond EP41S-1HT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a 100 to 30 mix ratio by weight and is formulated to..
Dielectric Strength 17.3 kV/mm

@Thickness 3.17 mm
440 kV/in

@Thickness 0.125 in
Master Bond EP21CLV Two Component Epoxy System
Product Description: Master Bond EP21CLV is a two component, lower viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting. It features easy handling a..
Dielectric Strength 17.3 kV/mm

@Thickness 3.17 mm
440 kV/in

@Thickness 0.125 in
Master Bond EP30ND Non-Drip, Dimensionally Stable Epoxy Adhesive
Description: Master Bond Polymer System EP30ND is a high viscosity, two component epoxy adhesive/sealant with a paste consistency. It will cure at room temperature or more rapidly at elevated temper..
Dielectric Strength 17.3 kV/mm
440 kV/in
Dow Corning 3-4241 DIELECTRIC TOUGH GEL KIT
Two-part, translucent green, RT or heat cure, UV indicator, long working time, tough primerless chemical adhesion, UL 94 V-1 flammability classification.Information provided by Dow Corning
Dielectric Strength 17.3 - 23.6 kV/mm
440 - 600 kV/in
Average value: 19.9 kV/mm Grade Count:33
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Dielectric Strength 17.3 kV/mm
440 kV/in
ASTM D149
Arlon 55279R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass
Dielectric Strength 17.3 kV/mm
440 kV/in
Resinlab® EP1026HP Epoxy Adhesive
Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan..
Dielectric Strength 17.3 kV/mm
440 kV/in
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin
Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1..
Dielectric Strength 17.3 kV/mm
440 kV/in
Resinlab® UR3005 Clear Two Part Urethane Elastomer
Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi..
Dielectric Strength 17.3 kV/mm
440 kV/in
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to..
Dielectric Strength 17.3 kV/mm
440 kV/in
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP1282 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat..
Dielectric Strength 17.3 kV/mm
440 kV/in
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy
Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi..
Dielectric Strength 17.3 kV/mm
439 kV/in
Short Time; ASTM D149
Plenco 50335 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform..
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill FR® PA6/6 GF25 FR NAT005 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized, High Flow and Lubri..