Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 8.57 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.230 - 1.80 J/cm²
1.09 - 8.57 ft-lb/in²
Average value: 0.703 J/cm² Grade Count:50
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Charpy Impact, Notched 0.100 - 1.80 J/cm²
0.476 - 8.57 ft-lb/in²
Average value: 0.967 J/cm² Grade Count:6
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Charpy Impact, Notched 0.200 - 1.80 J/cm²
0.952 - 8.57 ft-lb/in²
Average value: 0.668 J/cm² Grade Count:57
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Charpy Impact, Notched 0.100 - 1.80 J/cm²
0.476 - 8.57 ft-lb/in²
Average value: 0.707 J/cm² Grade Count:60
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Charpy Impact, Notched 0.200 - 1.80 J/cm²
0.952 - 8.57 ft-lb/in²
Average value: 0.701 J/cm² Grade Count:44
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Charpy Impact, Notched 0.300 - 1.80 J/cm²
1.43 - 8.57 ft-lb/in²
Average value: 0.961 J/cm² Grade Count:19
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Charpy Impact, Notched 0.200 - 1.80 J/cm²
0.952 - 8.57 ft-lb/in²
Average value: 0.617 J/cm² Grade Count:27
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact, Notched 0.400 - 1.80 J/cm²
1.90 - 8.57 ft-lb/in²
Average value: 0.840 J/cm² Grade Count:51
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Charpy Impact, Notched 0.500 - 1.80 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 8.57 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.10 J/cm² Grade Count:11
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Charpy Impact, Notched 0.200 - 1.80 J/cm²
0.952 - 8.57 ft-lb/in²
Average value: 0.953 J/cm² Grade Count:60
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Charpy Impact, Notched 0.500 - 1.80 J/cm²
2.38 - 8.57 ft-lb/in²
Average value: 0.945 J/cm² Grade Count:10
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Charpy Impact, Notched 0.500 - 1.80 J/cm²

@Temperature -30.0 - 30.0 °C
2.38 - 8.57 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.11 J/cm² Grade Count:24
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact, Notched 0.500 - 1.80 J/cm²

@Temperature -30.0 - 30.0 °C
2.38 - 8.57 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 0.993 J/cm² Grade Count:7
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 0.900 - 1.80 J/cm²
4.28 - 8.57 ft-lb/in²
Average value: 1.35 J/cm² Grade Count:6
Overview of materials for Nylon, Amorphous Transparent Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value..
Charpy Impact, Notched 1.20 - 1.80 J/cm²

@Temperature -30.0 - -30.0 °C
5.71 - 8.57 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.34 J/cm² Grade Count:33
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Charpy Impact, Notched 1.20 - 1.80 J/cm²

@Thickness 3.00 - 3.00 mm
5.71 - 8.57 ft-lb/in²

@Thickness 0.118 - 0.118 in
Average value: 1.34 J/cm² Grade Count:33
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Charpy Impact, Notched 0.200 - 1.80 J/cm²
0.952 - 8.57 ft-lb/in²
Average value: 0.592 J/cm² Grade Count:9
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..