Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 57.5 - 57.5 MPa

@Temperature 130 - 175 °C
8340 - 8340 psi

@Temperature 266 - 347 °F
Average value: 53.8 MPa Grade Count:1
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Tensile Strength, Ultimate 57.5 - 57.5 MPa

@Time 1.80e+7 - 7.20e+7 sec
8340 - 8340 psi

@Time 5000 - 20000 hour
Average value: 53.8 MPa Grade Count:1
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..