Polymer Property : Izod Impact, Notched = 0.69407 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.69407 - 1.6017 J/cm

@Temperature -40.0 - -30.0 °C
1.3003 - 3.0006 ft-lb/in

@Temperature -40.0 - -22.0 °F
Average value: 1.03 J/cm Grade Count:11
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched 0.69407 - 1.81526 J/cm

@Temperature -40.0 - 0.000 °C
1.3003 - 3.40073 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 1.11 J/cm Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Izod Impact, Notched 0.69407 - 1.81526 J/cm

@Thickness 3.17 - 3.20 mm
1.3003 - 3.40073 ft-lb/in

@Thickness 0.125 - 0.126 in
Average value: 1.11 J/cm Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Izod Impact, Notched 0.69407 - 0.69407 J/cm

@Temperature -40.0 - -40.0 °C
1.3003 - 1.3003 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.05 J/cm Grade Count:1
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Notched 0.69407 - 0.69407 J/cm

@Temperature -40.0 - -40.0 °C
1.3003 - 1.3003 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.694 J/cm Grade Count:1
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Copyright © lookpolymers.com All Rights Reserved