Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.5339 - 1.0678 J/cm @Temperature -40.0 - -30.0 °C |
1.000 - 2.0004 ft-lb/in @Temperature -40.0 - -22.0 °F |
Average value: 0.774 J/cm Grade Count:4 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Izod Impact, Notched | 0.500 - 1.0678 J/cm @Temperature -29.0 - 0.000 °C |
0.937 - 2.0004 ft-lb/in @Temperature -20.2 - 32.0 °F |
Average value: 0.784 J/cm Grade Count:2 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Temperature -40.0 - -40.0 °C |
2.0004 - 2.0004 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.05 J/cm Grade Count:9 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Thickness 3.17 - 3.17 mm |
2.0004 - 2.0004 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.05 J/cm Grade Count:9 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Temperature -40.0 - -40.0 °C |
2.0004 - 2.0004 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.850 J/cm Grade Count:2 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Thickness 3.17 - 3.17 mm |
2.0004 - 2.0004 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 0.850 J/cm Grade Count:2 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Temperature -40.0 - -40.0 °C |
2.0004 - 2.0004 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.07 J/cm Grade Count:9 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Thickness 3.17 - 3.17 mm |
2.0004 - 2.0004 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.07 J/cm Grade Count:9 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |