Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Plastiblend® PC/ABS 2110 BK

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Techmer ES Plastiblend® PC/ABS 2110 BK.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 0.10 %
<br>@Time 86400 sec
0.10 %
<br>@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm
<br>@Thickness 3.17 mm
0.0060 in/in
<br>@Thickness 0.125 in
ASTM D955
Melt Flow 5.5 g/10 min
<br>@Load 3.80 kg,<br> Temperature 230 °C
5.5 g/10 min
<br>@Load 8.38 lb,<br> Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Elongation at Break 130 %
130 %
ASTM D638
Flexural Yield Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 3.74 J/cm
<br>@Thickness 3.17 mm,<br> Temperature -40.0 °C
7.00 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature -40.0 °F
ASTM D256
4.81 J/cm
<br>@Thickness 3.17 mm,<br> Temperature -30.0 °C
9.00 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature -22.0 °F
ASTM D256
5.87 J/cm
<br>@Thickness 3.17 mm,<br> Temperature 22.8 °C
11.0 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.8 µm/m-°C
41.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
219 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB