Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.40 J/cm²

@Temperature -40.0 °C
11.4 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 FK 2010 Nylon 6.6 for injection molding, 20% glass fiber and 10% glass ball reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.40 J/cm²

@Temperature -40.0 °C
11.4 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 HH-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.40 J/cm²
11.4 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 HH-KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.40 J/cm²
11.4 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 HH-KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.40 J/cm²

@Temperature -40.0 °C
11.4 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 SG30 Nylon 6.6 for injection molding, 30% mineral filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.40 J/cm²

@Temperature -40.0 °C
11.4 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL C73 H-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced
Nylon 6.6/6 for injection molding, medium viscosity, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.40 J/cm²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Nilit Nilamid A G5 FR C4 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Halogens)
Description: Nilamid A G5 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ..
Charpy Impact Unnotched 2.40 J/cm²
11.4 ft-lb/in²
ISO 179/1eU
Nilit FRIANYL A63 BR80 Nylon 6.6 for injection molding, 80% bronze filled
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.40 J/cm²
11.4 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.40 J/cm²
11.4 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.40 J/cm²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Nilit FRIANYL A63 V0 G5 Nylon 6.6 for injection molding, 25% glass fiber reinforced
Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.40 J/cm² - NB
11.4 ft-lb/in² - NB
Average value: 16.1 J/cm² Grade Count:94
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Charpy Impact Unnotched 2.40 J/cm² - NB

@Temperature -40.0 - 30.0 °C
11.4 ft-lb/in² - NB

@Temperature -40.0 - 86.0 °F
Average value: 5.44 J/cm² Grade Count:35
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Charpy Impact Unnotched 2.40 - 9.00 J/cm²

@Temperature -40.0 - -20.0 °C
11.4 - 42.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.51 J/cm² Grade Count:28
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Charpy Impact Unnotched 2.40 J/cm²
11.4 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo..
Charpy Impact Unnotched 2.40 J/cm²
11.4 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1850-7557 PBT, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour, self-lubricating, for highest tribologic needs.Low warpag..
Charpy Impact Unnotched 2.40 J/cm²
11.4 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
Charpy Impact Unnotched 2.40 J/cm²

@Temperature -30.0 °C
11.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/2C
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
Charpy Impact Unnotched 2.40 J/cm²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DSM Arnite® B600SE PBT FR
Flame Retardant
Charpy Impact Unnotched 2.40 J/cm²
11.4 ft-lb/in²
ISO 179
Chi Mei Kibisan® PN-127H SAN
Chemical Resistant
Charpy Impact Unnotched 2.40 - 6.50 J/cm²
11.4 - 30.9 ft-lb/in²
Average value: 5.20 J/cm² Grade Count:7
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced