Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 140 - 150 cm³/g | 140 - 150 cm³/g | Average value: 144 cm³/g Grade Count:5 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Viscosity Test | 140 - 150 cm³/g | 140 - 150 cm³/g | Average value: 143 cm³/g Grade Count:3 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Viscosity Test | 140 - 150 cm³/g | 140 - 150 cm³/g | Average value: 145 cm³/g Grade Count:4 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Viscosity Test | 140 - 150 cm³/g | 140 - 150 cm³/g | Average value: 147 cm³/g Grade Count:4 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, good heat-ageing resistance |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® BKV 25 H2.0 LT 904040 Nylon 6, 25% Glass Fiber PA 6, injection molding grade, 25% glass fibers, good heat-ageing resistance, laser-weldable |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s.. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® BKV 30 HTS 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, very good heat-ageing resistance |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® DP 2131/20 W1 901317 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, weather resistance, good heat-ageing resistance |
|||
Viscosity Test | 140 - 160 cm³/g | 140 - 160 cm³/g | Sulphuric Acid; EN ISO 307 |
Domo Domamid® 39 APBH Polyamide 6.6 DOMAMID® 39APBH are Polyamide 6.6 pellets produced from AH-salt.Applications: Injection moulding CompoundingExtrusionInformation provided by Domo |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) 25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p.. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6
(Unverified Data**) 15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per.. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307 |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Conditioned) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307 |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307 |
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Dry) Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307 |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number |
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned) Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® BKV 35 H2.0 901510 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: automotive structures |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® B 1600 000000 PBT PBT, non-reinforced, injection molding, extrusion, food contact |
|||
Viscosity Test | 140 - 150 cm³/g | 140 - 150 cm³/g | Average value: 148 cm³/g Grade Count:8 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307 |
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307 |
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry) Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade. |
|||
Viscosity Test | 140 cm³/g | 140 cm³/g | Viscosity number; ISO 307 |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |