Polymer Property : Compressive Yield Strength = 172 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 3.00 - 172 MPa
435 - 24900 psi
Average value: 51.2 MPa Grade Count:33
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Compressive Yield Strength 62.1 - 172 MPa
9000 - 24900 psi
Average value: 119 MPa Grade Count:14
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Compressive Yield Strength 89.6 - 172 MPa
13000 - 24900 psi
Average value: 122 MPa Grade Count:3
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Compressive Yield Strength 131 - 172 MPa
19000 - 25000 psi
Average value: 145 MPa Grade Count:3
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Compressive Yield Strength 152 - 172 MPa
22000 - 25000 psi
Average value: 164 MPa Grade Count:4
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Compressive Yield Strength 89.6 - 172 MPa
13000 - 25000 psi
Average value: 134 MPa Grade Count:12
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..