Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.320 J/cm

@Temperature 23.0 °C
0.600 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products HP514-01 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.320 J/cm

@Temperature 23.0 °C
0.600 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.320 J/cm

@Temperature 23.0 °C
0.600 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products M15P101-01A 15% Mica Reinforced Polypropylene, Black
Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256 Type A
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)
Izod Impact, Notched 0.320 J/cm

@Thickness 3.20 mm,
Temperature 22.8 °C
0.600 ft-lb/in

@Thickness 0.126 in,
Temperature 73.0 °F
injection molded ASTM Type 1 specimen; ASTM D256
Pinnacle Polymers 1120 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
Izod Impact, Notched 0.320 J/cm

@Thickness 6.35 mm
0.600 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Plaskolite West Optix® CP - 924 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 4000 AR 30  Polyphthalamide (PPA) Aramid Fiber 30%  (discontinued **)
Aramid Fiber 30%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Izod Impact, Notched 0.320 J/cm

@Temperature 23.0 °C
0.600 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black
Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products  (discontinued **)
ENSITEP is an unreinforced, semi-crystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and ..
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Quantum Nylon 6/6
Information provided by Quantum Advanced Engineering Plastics
Izod Impact, Notched 0.320 - 2.40 J/cm
0.600 - 4.50 ft-lb/in
Average value: 0.882 J/cm Grade Count:64
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Global PEI-110 Easy Flow, Polyetherimide
Information provided by Global Polymers Corporation.
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Techmer ES Electrafil® NY-3/EC BK PA6
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PA6/6 FR HS BK (Dry)
Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PP GB50 50% Glass Beads Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 50% Filler by WeightInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Luriblend® PA6/6 04003 Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizedAppearance: Natu..
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Luriblend® PA6/6 TL20 HS L Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant(20%)Features: Lubricated, Heat Stabilized and Good Wear ResistanceInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Luriblend® PBT GB30 TL15 30% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Techmer ES Plaslube® J-1/CF/10/TF/13/SI/2 NAT PA66
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene
DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf..
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Washington Penn Homopolymer Polypropylene
Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array ..
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Washington Penn Homopolymer Polypropylene 50% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 150 HF Polypropylene (PP), High Flow - Unreinforced - Flame Retardant - UL94 V-0
RTP 150 HF is a low viscosity, flame retardant, unreinforced polypropylene material which possesses UL94 flammability and elevated RTI ratings. RTP 150 HF offers excellent moldability with the livi..
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Formosa Plastics Formolene® 4142R Injection Molding Polypropylene
Homopolymer with Nucleating, Antistat AdditivesApplications: Appliance, closure and thin wall applications.Formolene 4142R is a low viscosity, highly isotactic polypropylene homopolymer designed pri..
Izod Impact, Notched 0.320 J/cm

@Thickness 3.20 mm
0.600 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 2099 X 126218 A Bio-Based Polylactic Acid (PLA); Impact Modified - 94% Renewable Resource Content
For detailed processing information, see the PLA Molding Guide on the RTP Company website.
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
molded and tested in accordance with ASTM D 4101; ASTM D256A
Dow 5E89 Polypropylene Resin
DOW 5E89 is intended for use in stretched tape (raffia) processes, from which the raffia is used to produce woven fabrics for carpet backing, sacking, industrial and geotextile applications.Informat..
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Ensinger Tecast Vekton™ 6PAL Oil-Filled Cast Nylon 6 (PA6)
Tecast® 6PAL is used in applications requiring excellent bearing and wear properties where external lubrication is difficult or impractical.General Tecast® Cast Nylon Information: Tecast cast nylo..
Izod Impact, Notched 0.320 - 1.17 J/cm
0.600 - 2.20 ft-lb/in
Average value: 0.830 J/cm Grade Count:20
Overview of materials for Polyphthalamide (PPA), Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 0.320 J/cm

@Temperature -40.0 °C
0.600 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Celanese Celcon® MC270-HM POM, Mineral Reinforced
Celcon« MC270-HM is a high modulus, mineral coupled acetal copolymer. It utilizes a higher additive level to provide significant improvement in product stiffness and mold shrinkage and better warp..