Polymer Property : Charpy Impact, Notched = 0.200 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Polycasa Acryl® G 87 E Acrylic
Grade for extruding semi-finished products such as twin-strapped panels, profile and tubes, as well as injection molding of watch glasses, dishes, bowls, water-tap hand grips and bathroom fittings, ..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 SG40 Nylon 6.6 for injection molding, 40% mineral filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.200 - 0.350 J/cm²
0.952 - 1.67 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group 4554 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi..
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is also a PPA resin.Information provided by DuPont Performan..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
DIN 53453
Nilit RECONYL A SG30 Recycled nylon 6.6 for injection molding, 30% mineral filled
Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures  (disconti
Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application ..
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eA
Hexion Bakelite™ PF 6506 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures, UL Listed &nbs
Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant, UL listed molding compound 1.5 mm/V-..
Charpy Impact, Notched 0.200 - 0.300 J/cm²

@Temperature -30.0 - -30.0 °C
0.952 - 1.43 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.250 J/cm² Grade Count:4
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
J/cm; ASTM D256
Plenco Valite 4100 Novolac Phenolic, Granular, Compression Molded  (discontinued **)
This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac..
Charpy Impact, Notched 0.200 - 1.70 J/cm²
0.952 - 8.09 ft-lb/in²
Average value: 0.635 J/cm² Grade Count:40
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179
Manifattura Cattaneo PET Polyethylene Terephthalate
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
LATI Laticonther 52/35 CP1/45 PP Homopolymer
High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
LATI Laticonther 62 GR/70 PA 6, 70% Graphite Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend (Asia Pacific)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.
Charpy Impact, Notched 0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Styrolution Luran® 378 P Crystal Clear Transparent SAN
Description: Easy-flow grade with enhanced resistance to chemicals.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179
Styrolution Luran® 358 N SAN
Luran 358 N is an easy-flowing injection molding SAN grade.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Charpy Impact, Notched 0.200 J/cm²

@Temperature -30.0 °C
0.952 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Styrolution Terlux® 2802 TR MABS
Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Charpy Impact, Notched 0.200 J/cm²

@Temperature -20.0 °C
0.952 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis Beta-PPR™ RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems
Beta-PPR RA7050 is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of t..
Charpy Impact, Notched 0.200 J/cm²

@Temperature -20.0 °C
0.952 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating
Borsoft SF203CF is a new statistic-heterophasic propylene-ethylene copolymer suitable for coating applications. Its polymer structure permits perfect adhesion to certain products. According to the..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179/1eA
Borealis Borstar® ME3440 Black Medium Density Polyethylene for Pressure Pipes
Borstar ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Bor..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ASTM D256
Plenco 2311 Phenolic, Granular, Compression Molded
PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 300FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, High Flow
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® L 20 EC PA12-CD25
Product Description: Grilamid L 20 EC is an electrically conductive, medium viscosity injection molding product, based on Polyamid 12 (PA12). Grilamid L 20 EC is heat stabilized, easy to process wit..
Charpy Impact, Notched 0.200 - 0.500 J/cm²

@Temperature -20.0 - 30.0 °C
0.952 - 2.38 ft-lb/in²

@Temperature -4.00 - 86.0 °F
Average value: 0.350 J/cm² Grade Count:5
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.200 - 1.00 J/cm²

@Temperature -30.0 - -20.0 °C
0.952 - 4.76 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.480 J/cm² Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO Data
Americas Styrenics Styron® 612 Polystyrene  (discontinued **)
STYRON® 612 general purpose polystyrene resin is an easy flow resin with no color additives. When used unmodified for the manufacture of food contact articles STYRON 612 complies with the US Food, ..
Charpy Impact, Notched 0.200 J/cm²

@Temperature 30.0 °C
0.952 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® G 16 PA6I/6T
Product description: Grivory G 16 is a low viscosity amorphous copolyamide. It is suitable for injection - stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of co..
Charpy Impact, Notched 0.200 - 0.460 J/cm²
0.952 - 2.19 ft-lb/in²
Average value: 0.323 J/cm² Grade Count:6
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..
Charpy Impact, Notched 0.200 - 2.60 J/cm²

@Thickness 102 - 102 mm
0.952 - 12.4 ft-lb/in²

@Thickness 4.00 - 4.00 in
Average value: 1.39 J/cm² Grade Count:7
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..
Copyright © lookpolymers.com All Rights Reserved