Polymer Property : Charpy Impact Unnotched = 2.00 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Polyplastic Armlen® PP MF 40-3M Polypropylene Copolymer, 40% Calcium Carbonate
Injection moldingInformation provided by PolyPlastic Group.
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -40.0 °C
9.52 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 HH-KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -40.0 °C
9.52 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 HH-KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eU
Celanese FORTRON 6165A4 PPS, 65% Mineral / Glass Reinforced  (Unverified Data**)
Fortron 6165A4 offers a unique balance of properties based on a high mineral and glass reinforced composition. The heat resistance under load bearing conditions is excellent for this product. As wit..
Charpy Impact Unnotched 2.00 J/cm² - NB
9.52 ft-lb/in² - NB
Average value: 6.08 J/cm² Grade Count:32
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6
Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
LATI LATILUB 73/13-20ST Polyoxymethylene Base (POM), 20% Mixed PTFE/Silicone Self Lubricating Plastic  (discon
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Charpy Impact Unnotched 2.00 - 999.9 J/cm²

@Temperature -30.0 - -30.0 °C
9.52 - 4759 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.94 J/cm² Grade Count:7
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
Charpy Impact Unnotched 2.00 J/cm² - NB

@Temperature -40.0 - -20.0 °C
9.52 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 6.01 J/cm² Grade Count:17
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Charpy Impact Unnotched 2.00 - 11.0 J/cm²

@Temperature -30.0 - 30.0 °C
9.52 - 52.4 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 7.73 J/cm² Grade Count:19
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301-7578 PPS, linear, with glass fiber and PTFE, improved wear resistance
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301-8077 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricity.S..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1850-8384 PBT, with carbon fiber, thermally conductive modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low waterabsorbtion.Electrically conductive, suitable for continuous discha..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 80-8106 Polyacetal-copolymer, with carbon fiber, PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® CLG902 Acrylic Polymer
Information provided by Lucite International
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS (Asia Pacific)
35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market.
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eU
Polyplastics TOPAS® 8007 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade)
Water adsorption is small and barrier properties are good, making this grade particularly suitable for package applications for products that dislike moisture. Grade 8007 has lower coefficient of el..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Topas Advanced Polymers TOPAS® 8007D-61 Cyclic Olefin Copolymer (COC)
TOPAS® 8007D-61 is an externally lubricated version of our 8007 series of injection molding resins, targeting injection blow molding (IBM) and injection stretch blow molding (ISBM) applications. Li..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Rynite® 515CS BK575M PET
Rynite® 515CS BK575M is a 15% glass fiber reinforced, black polyethylene terephthalate resin modified for improved color stability after heat aging.Information provided by DuPont Performance Polyme..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179-1eU
Barlog Plastics KEBATRON L1065X3 PPS, linear, 65% glass fiber / mineral reinforced
PPS-GF/MD 65Information provided by BARLOG plastics GmbH.
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese CELANEX 3200FC PBT, 15% Glass Reinforced
Celanex 3200FC is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 30.0 °C
9.52 ft-lb/in²

@Temperature 86.0 °F
ISO 179/1eU
Celanese Celanex® 3200 PBT, 15% Glass Reinforced
Celanex 3200 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.To avoid hydrolytic degradation during processing, ..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese ZENITE 6140L LCP, 40% Glass Reinforced
Zenite« 6140L is a 40% glass fiber reinforced and lubricated liquid crystal polymer for injection molding. It has excellent impact resistance and excellent heat deflection temperature.Information p..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
Arkema Group Oroglas® V 825 T Acrylic  (discontinued **)
OROGLAS V 825 T exhibits an excellent balance of properties including superior thermal resistance with an easy processing behavior.OROGLAS V 825 T is then the material of choice for automotive appli..
Charpy Impact Unnotched 2.00 - 4.00 J/cm²

@Temperature -40.0 - -30.0 °C
9.52 - 19.0 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 3.07 J/cm² Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® A 218 S30 Black 21 N PA66, 30% glass fiber, DRY
Description: Polyamide PA66, reinforced with 30% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 218 S30 is used in all sectors of indu..
Charpy Impact Unnotched 2.00 - 3.00 J/cm²

@Temperature -20.0 - -20.0 °C
9.52 - 14.3 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 2.45 J/cm² Grade Count:8
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Charpy Impact Unnotched >= 2.00 J/cm²
>= 9.52 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR F 4206 Bulk Molding Compound
General purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), ther..