PRODUCT NO. Category Trade Name
Unitika A1022GFL15 PA6, 15% Glass Fiber Reinforced, Conditioned Nylon 6, 20% Glass Fiber Filled
Unitika A1022GFL15 PA6, 15% Glass Fiber Reinforced, Dry Nylon 6, 20% Glass Fiber Filled
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Conditioned Nylon 6, 60% Glass Fiber Filled
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Dry Nylon 6, 60% Glass Fiber Filled
Unitika A1025GO PA6, Flame Retardant, Conditioned Nylon 6, Unreinforced, Flame Retardant
Unitika A1025NO PA6, Flame Retardant, Conditioned Nylon 6, Unreinforced, Flame Retardant
Unitika A1025NO PA6, Flame Retardant, Dry Nylon 6, Unreinforced, Flame Retardant
Unitika A1030BRL PA6, Conditioned Nylon 6, Unreinforced
Unitika A1030BRL PA6, Dry Nylon 6, Unreinforced
Unitika A1030FR PA6, Conditioned Nylon 6, Unreinforced
Unitika A1030FR PA6, Dry Nylon 6, Unreinforced
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Conditioned Nylon 6, 30% Glass Fiber Filled
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry Nylon 6, 30% Glass Fiber Filled
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Conditioned Nylon 6, 50% Glass Fiber Filled
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Dry Nylon 6, 50% Glass Fiber Filled
Unitika A1030JR PA6, Conditioned Nylon 6, Unreinforced
Unitika A1030SR PA6, Dry Nylon 6, Unreinforced
Unitika A1030TF PA6, Conditioned Nylon 6, Unreinforced
Unitika A125 PA66, Conditioned Nylon 66, Unreinforced
Unitika A125 PA66, Dry Nylon 66, Unreinforced
Unitika A175G15 PA66, 15% Glass Fiber Reinforced, Conditioned Nylon 66, 20% Glass Fiber Filled
Unitika A175G15 PA66, 15% Glass Fiber Reinforced, Dry Nylon 66, 20% Glass Fiber Filled
Unitika A3030N-2 PA6, 30% Mineral Reinforced, Conditioned Nylon 6, 40% Mineral Filled
Unitika A3030N-2 PA6, 30% Mineral Reinforced, Dry Nylon 6, 40% Mineral Filled
Unitika A3130 PA6, 35% Mineral Reinforced, Conditioned Nylon 6, 40% Mineral Filled
Unitika A3130 PA6, 35% Mineral Reinforced, Dry Nylon 6, 40% Mineral Filled
Unitika A3130HR-25 PA6, 25% Mineral Reinforced, Conditioned Nylon 6, 30% Mineral Filled
Unitika A3130HR-25 PA6, 25% Mineral Reinforced, Dry Nylon 6, 30% Mineral Filled
Unitika AX-1500 Conditioned Polyarylate
Unitika AX-1500 Dry Polyarylate
Unitika AX-1500W Conditioned Polyarylate
Unitika AX-1500W Dry Polyarylate
Unitika AXF-1500-05 Conditioned Polyarylate
Unitika AXF-1500-05 Dry Polyarylate
Unitika AXG-1500-300 Conditioned Polyarylate
Unitika AXG-1500-300 Dry Polyarylate
Unitika B2040G33 PA66, 33% Glass Fiber Reinforced, Conditioned Nylon 66, 30% Glass Fiber Filled
Unitika B2040G33 PA66, 33% Glass Fiber Reinforced, Dry Nylon 66, 30% Glass Fiber Filled
Unitika B2040G50 PA66, 50% Glass Fiber Reinforced, Conditioned Nylon 66, 50% Glass Fiber Filled
Unitika B2040G50 PA66, 50% Glass Fiber Reinforced, Dry Nylon 66, 50% Glass Fiber Filled
Unitika BV2120 PA66, Flame Retardant, Dry Nylon 66, Unreinforced, Flame Retardant
Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Conditioned Nylon 66, Glass Fiber Filled, Flame Retardant
Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Dry Nylon 66, Glass Fiber Filled, Flame Retardant
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Conditioned Nylon 66, Glass Fiber Filled, Flame Retardant
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Dry Nylon 66, Glass Fiber Filled, Flame Retardant
Unitika C300VN Polyarylate
Unitika CX-2500 PA6, Conditioned Nylon 6, Unreinforced
Unitika elitel UE3200 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3201 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3203 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3210 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3215 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3220 Polyester, Flake Polyester, TP elitel
Unitika elitel UE3223 Polyester, Flake Polyester, TP elitel
Unitika elitel UE3230 Polyester, Flake Polyester, TP elitel
Unitika elitel UE3231 Polyester, Flake Polyester, TP elitel
Unitika elitel UE3240 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3250 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3300 Polyester, Flake Polyester, TP elitel
Unitika elitel UE3320 Polyester, Flake Polyester, TP elitel
Unitika elitel UE3350 Polyester, Flake Polyester, TP elitel
Unitika elitel UE3370 Polyester, Flake Polyester, TP elitel
Unitika elitel UE3380 Polyester, Flake Polyester, TP elitel
Unitika elitel UE3400 Polyester, Flake Polyester, TP elitel
Unitika elitel UE9600 Polyester, Pellet Polyester, TP elitel
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Conditioned Nylon 66, 60% Glass Fiber Filled
Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Dry Nylon 66, 60% Glass Fiber Filled
Unitika E-RUNG60 Ultra high-rigidity PA6, Conditioned Nylon 6
Unitika EX-1020K PA6, Conditioned Nylon 6, Unreinforced
Unitika EX-1222 PA6, Dry Nylon 6, Impact Grade
Unitika L-1003PA Polyarylate
Unitika LM-8503-10 Polyarylate
Unitika M1030B PA6, Conditioned Nylon 6
Unitika M1030B PA6, Dry Nylon 6
Unitika M1030DH PA6, Dry Nylon 6
Unitika M1030E PA6, Dry Nylon 6
Unitika M2350 PA6, Conditioned Nylon 6
Unitika P-1001 Engineering Plastic Polyarylate
Unitika P-3001S Engineering Plastic Polyarylate
Unitika P-5001 Engineering Plastic Polyarylate
Unitika RUN35-C25 PA6, Conditioned Nylon 6
Unitika RUN35-C25 PA6, Dry Nylon 6
Unitika RUN35-TA Light resistant PA6, Dry Nylon 6
Unitika TERRAMAC TE-8210 Polylactic Acid (PLA) Polylactic Acid (PLA) Biopolymer TERRAMAC
Unitika U-8400H Polyarylate
Unitika UG-100-20 Engineering Plastic Polyarylate
Unitika A1025GO PA6, Flame Retardant, Dry Nylon 6, Unreinforced, Flame Retardant
Unitika A1030JR PA6, Dry Nylon 6, Unreinforced
Unitika A1030SR PA6, Conditioned Nylon 6, Unreinforced
Unitika A1030TF PA6, Dry Nylon 6, Unreinforced
Unitika CX-2500 PA6, Dry Nylon 6, Unreinforced
Unitika elitel UE3216 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3620 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3660 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3690 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3700 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE3800 Polyester, Pellet Polyester, TP elitel
Unitika elitel UE9200 Polyester, Pellet Polyester, TP elitel
Unitika E-RUNG60 Ultra high-rigidity PA6, Dry Nylon 6
Unitika ET2025 PA6, Conditioned Nylon 66, Impact Grade