| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 2.3 % | 2.3 % | 50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.016 cm/cm @Thickness 3.20 mm |
0.016 in/in @Thickness 0.126 in |
|
| Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Thickness 3.20 mm |
0.022 in/in @Thickness 0.126 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 108 | 108 | ISO 2039 |
| Tensile Strength, Yield | 60.0 MPa | 8700 psi | ISO 527-1/-2 |
| Elongation at Break | >= 100 % | >= 100 % | ISO 527-1/-2 |
| Tensile Modulus | 1.00 GPa | 145 ksi | ISO 527-1/-2 |
| Flexural Strength | 43.0 MPa | 6240 psi | ISO 178 |
| Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
| Charpy Impact Unnotched | NB | NB | ISO 179-1 |
| Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-2 |
| Flammability, UL94 | V-2 @Thickness 0.810 mm |
V-2 @Thickness 0.0319 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |