| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | Unitika |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Unitika RUN35-TA Light resistant PA6, Dry.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
| Moisture Absorption at Equilibrium | 0.93 % | 0.93 % | 50% RH |
| Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 88 | 88 | ASTM D785 |
| Tensile Strength at Break | 141 MPa | 20500 psi | ASTM D638 |
| Elongation at Break | 2.9 % | 2.9 % | ASTM D638 |
| Tensile Modulus | 19.4 GPa | 2810 ksi | ASTM D638 |
| Flexural Strength | 215 MPa | 31200 psi | ASTM D790 |
| Flexural Modulus | 17.8 GPa | 2580 ksi | ASTM D790 |
| Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 1.40 µm/m-°C | 0.778 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 183 °C | 361 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 205 °C | 401 °F | ASTM D648 |