Material Notes:
Adhesive agent, Resin modifier, Good solubility, Low temperature sealingUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binders, and modifying agents to the products in new-generation high-tech fields.Characteristics:l products have superior adhesiveness and coatability. They exhibit excellent adhesiveness and coatability to films and molded products of plastic materials such as polyester, polyvinylchloride, polycarbonate, and cellulose acetate; steel materials such as steel plates; metal materials such as copper, and aluminum; woven or nonwoven fabrics from polyester and other fibers; papers, woods, and others.l products may be hardened by combined use of a hardening agent.Blending of an l resin with another l resin or a different resin provides alloys with more diversified resin properties. Additionally, l products are effective as a modifying resin for providing other resins with flexibility, coatability, toughness, and others. l resins form films excellent in flexibility, electrical properties, weather resistance, as well in appearance and transparency: l resins retain consistent quality with smaller change in quality over time They are also excellent hygienically.Information provided by Unitika Ltd.
Physical Properties Metric English Comments
Moisture Absorption at Equilibrium 0.50 %
0.50 %
60%RH
Molecular Weight 21000 g/mol
21000 g/mol
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 1.00 °C
33.8 °F
Chemical Properties Metric English Comments
Acid Value 1.0
1.0
[mgKOH/g}
Descriptive Properties Value Comments
Appearance Pale yellow
Hydroxyl Value 8 mgKOH/g