Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polypropylene with 40% Glass Fiber Filler

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polypropylene with 40% Glass Fiber Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.09 - 1.56 g/cc
0.0394 - 0.0564 lb/in³
Average value: 1.22 g/cc Grade Count:149
Filler Content 35.0 - 45.0 %
35.0 - 45.0 %
Average value: 39.6 % Grade Count:53
Water Absorption 0.0100 - 0.0700 %
0.0100 - 0.0700 %
Average value: 0.0417 % Grade Count:23
Additive Loading 40.0 %
40.0 %
Average value: 40.0 % Grade Count:3
Linear Mold Shrinkage 0.000300 - 0.0350 cm/cm
0.000300 - 0.0350 in/in
Average value: 0.00325 cm/cm Grade Count:111
Linear Mold Shrinkage, Transverse 0.00500 - 0.0165 cm/cm
0.00500 - 0.0165 in/in
Average value: 0.00972 cm/cm Grade Count:9
Melt Flow 1.00 - 25.0 g/10 min
1.00 - 25.0 g/10 min
Average value: 5.63 g/10 min Grade Count:81
Spiral Flow 106 - 106 cm

@Temperature 250 - 250 °C
41.7 - 41.7 in

@Temperature 482 - 482 °F
Average value: 106 cm Grade Count:1
106 - 106 cm

@Thickness 2.00 - 2.00 mm
41.7 - 41.7 in

@Thickness 0.0787 - 0.0787 in
Average value: 106 cm Grade Count:1
Ash 28.0 - 40.0 %
28.0 - 40.0 %
Average value: 38.5 % Grade Count:6
Mechanical Properties Metric English Comments
Hardness, Rockwell M 58.0 - 72.0
58.0 - 72.0
Average value: 62.5 Grade Count:4
Hardness, Rockwell R 82.0 - 116
82.0 - 116
Average value: 105 Grade Count:34
Hardness, Shore D 74.0 - 85.0
74.0 - 85.0
Average value: 76.6 Grade Count:17
Tensile Strength, Ultimate 30.0 - 150 MPa
4350 - 21800 psi
Average value: 96.4 MPa Grade Count:97
60.0 - 175.816 MPa

@Temperature -40.0 - 93.3 °C
8700 - 25500.0 psi

@Temperature -40.0 - 200 °F
Average value: 80.8 MPa Grade Count:16
Tensile Strength, Yield 40.5 - 125 MPa
5870 - 18100 psi
Average value: 89.3 MPa Grade Count:61
48.0 - 48.0 MPa

@Temperature 100 - 100 °C
6960 - 6960 psi

@Temperature 212 - 212 °F
Average value: 48.0 MPa Grade Count:1
Elongation at Break 1.00 - 10.0 %
1.00 - 10.0 %
Average value: 3.23 % Grade Count:107
1.80 - 5.50 %

@Temperature 4.44 - 100 °C
1.80 - 5.50 %

@Temperature 40.0 - 212 °F
Average value: 2.48 % Grade Count:17
Elongation at Yield 1.00 - 6.70 %
1.00 - 6.70 %
Average value: 3.53 % Grade Count:32
Modulus of Elasticity 3.59 - 12.4 GPa
520 - 1800 ksi
Average value: 8.31 GPa Grade Count:76
4.50 - 11.6521 GPa

@Temperature -40.0 - 100 °C
653 - 1690.03 ksi

@Temperature -40.0 - 212 °F
Average value: 6.55 GPa Grade Count:17
Flexural Yield Strength 50.0 - 241 MPa
7250 - 35000 psi
Average value: 143 MPa Grade Count:123
85.0 - 293.717 MPa

@Temperature -40.0 - 93.3 °C
12300 - 42600.1 psi

@Temperature -40.0 - 200 °F
Average value: 127 MPa Grade Count:14
Flexural Modulus 2.80 - 12.5 GPa
406 - 1810 ksi
Average value: 7.10 GPa Grade Count:153
4.44022 - 11.3763 GPa

@Temperature -40.0 - 121 °C
644.010 - 1650.03 ksi

@Temperature -40.0 - 250 °F
Average value: 6.48 GPa Grade Count:13
Compressive Yield Strength 61.4 - 86.2 MPa
8900 - 12500 psi
Average value: 69.6 MPa Grade Count:3
Izod Impact, Notched 0.427 - 7.52 J/cm
0.800 - 14.1 ft-lb/in
Average value: 1.32 J/cm Grade Count:112
0.500 - 3.84408 J/cm

@Temperature -40.0 - 93.3 °C
0.937 - 7.20154 ft-lb/in

@Temperature -40.0 - 200 °F
Average value: 1.61 J/cm Grade Count:5
Izod Impact, Unnotched 1.49 - 9.08 J/cm
2.79 - 17.0 ft-lb/in
Average value: 5.61 J/cm Grade Count:42
3.70 - 3.70 J/cm

@Temperature -40.0 - -40.0 °C
6.93 - 6.93 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 3.70 J/cm Grade Count:2
Izod Impact, Notched (ISO) 10.0 - 26.0 kJ/m²
4.76 - 12.4 ft-lb/in²
Average value: 18.7 kJ/m² Grade Count:7
10.0 - 23.0 kJ/m²

@Temperature -30.0 - -20.0 °C
4.76 - 10.9 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 16.0 kJ/m² Grade Count:3
Charpy Impact Unnotched 1.50 - 8.00 J/cm²
7.14 - 38.1 ft-lb/in²
Average value: 5.53 J/cm² Grade Count:33
3.80 - 8.20 J/cm²

@Temperature -30.0 - -20.0 °C
18.1 - 39.0 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 5.43 J/cm² Grade Count:27
Charpy Impact, Notched 0.300 - 4.50 J/cm²
1.43 - 21.4 ft-lb/in²
Average value: 2.14 J/cm² Grade Count:42
0.400 - 3.60 J/cm²

@Temperature -30.0 - -20.0 °C
1.90 - 17.1 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 2.14 J/cm² Grade Count:29
Gardner Impact 0.113 - 1.13 J
0.0830 - 0.830 ft-lb
Average value: 0.476 J Grade Count:26
Dart Drop, Total Energy 6.34 - 15.5 J
4.68 - 11.4 ft-lb
Average value: 12.6 J Grade Count:3
5.76 - 13.7 J

@Temperature -20.0 - -20.0 °C
4.25 - 10.1 ft-lb

@Temperature -4.00 - -4.00 °F
Average value: 9.73 J Grade Count:1
5.76 - 13.7 J

@Thickness 3.18 - 3.18 mm
4.25 - 10.1 ft-lb

@Thickness 0.125 - 0.125 in
Average value: 9.73 J Grade Count:1
Thermal Properties Metric English Comments
CTE, linear 20.0 - 50.0 µm/m-°C
11.1 - 27.8 µin/in-°F
Average value: 32.5 µm/m-°C Grade Count:19
Thermal Conductivity 0.346 - 0.360 W/m-K
2.40 - 2.50 BTU-in/hr-ft²-°F
Average value: 0.355 W/m-K Grade Count:3
Melting Point 160 - 182 °C
320 - 360 °F
Average value: 165 °C Grade Count:33
Maximum Service Temperature, Air 65.0 - 140 °C
149 - 284 °F
Average value: 113 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 120 - 166 °C
248 - 331 °F
Average value: 158 °C Grade Count:80
Deflection Temperature at 1.8 MPa (264 psi) 65.0 - 175 °C
149 - 347 °F
Average value: 149 °C Grade Count:125
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 - 3.00e+16 ohm-cm
1.00e+14 - 3.00e+16 ohm-cm
Average value: 8.08e+15 ohm-cm Grade Count:16
Dielectric Constant 2.75 - 3.20
2.75 - 3.20
Average value: 3.03 Grade Count:5
Dielectric Strength 19.7 - 25.0 kV/mm
500 - 635 kV/in
Average value: 21.1 kV/mm Grade Count:11
Dissipation Factor 0.00100 - 0.00200
0.00100 - 0.00200
Average value: 0.00140 Grade Count:5
Arc Resistance 102 - 122 sec
102 - 122 sec
Average value: 109 sec Grade Count:3
Users viewing this material also viewed the following: