Polymer Property : Electrical Resistivity = 3.00e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 - 3.00e+16 ohm-cm
1.00e+13 - 3.00e+16 ohm-cm
Average value: 8.06e+15 ohm-cm Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Electrical Resistivity 1.00e+12 - 3.00e+16 ohm-cm
1.00e+12 - 3.00e+16 ohm-cm
Average value: 1.14e+16 ohm-cm Grade Count:14
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E..
Electrical Resistivity 1000 - 3.00e+16 ohm-cm
1000 - 3.00e+16 ohm-cm
Average value: 7.45e+15 ohm-cm Grade Count:11
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..
Electrical Resistivity 1.00e+15 - 3.00e+16 ohm-cm
1.00e+15 - 3.00e+16 ohm-cm
Average value: 1.16e+16 ohm-cm Grade Count:7
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max..
Electrical Resistivity 5.30e+15 - 3.00e+16 ohm-cm
5.30e+15 - 3.00e+16 ohm-cm
Average value: 2.18e+16 ohm-cm Grade Count:3
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..
Electrical Resistivity 1.00e+14 - 3.00e+16 ohm-cm
1.00e+14 - 3.00e+16 ohm-cm
Average value: 1.00e+16 ohm-cm Grade Count:10
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
Electrical Resistivity 1000 - 3.00e+16 ohm-cm
1000 - 3.00e+16 ohm-cm
Average value: 3.87e+15 ohm-cm Grade Count:28
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..
Electrical Resistivity 1.00e+14 - 3.00e+16 ohm-cm
1.00e+14 - 3.00e+16 ohm-cm
Average value: 8.08e+15 ohm-cm Grade Count:16
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..