Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 6.93 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
6.93 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
PolyOne Gravi-Tech™ GT6000-0023 Black Polyamide 6 (Nylon 6)
Information provided by PolyOne
Izod Impact, Unnotched 3.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
6.93 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D4812
PolyOne Geon™ 83510 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Unnotched 3.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
6.93 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
PolyOne Gravi-Tech™ GRV-NP-110-W-NAT Polyamide 12 (Nylon 12)
Information provided by PolyOne
Izod Impact, Unnotched 3.70 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
6.93 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® 12-031  (discontinued **)
PRE-ELEC 12-031 is a conductive thermoplastic compound based on a polyacetal copolymer with 10% carbon fiber. PRE-ELEC 12-031 exhibits excellent mechanical properties and electrical conductivity. Te..
Izod Impact, Unnotched 3.70 J/cm
6.93 ft-lb/in
ASTM D256
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to..
Izod Impact, Unnotched 3.70 J/cm
6.93 ft-lb/in
ASTM D256
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System
0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Izod Impact, Unnotched 3.70 J/cm

@Temperature -40.0 °C
6.93 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Adell ER-19 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness
Data provided by Adell Plastics, Inc.
Izod Impact, Unnotched 3.70 J/cm

@Temperature -40.0 °C
6.93 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Adell ER-39 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness
Data provided by Adell Plastics, Inc.
Izod Impact, Unnotched 3.70 J/cm
6.93 ft-lb/in
ASTM D256
Adell RA-16 Copolymer Polypropylene, 30% Talc Filled
Data provided by Adell Plastics, Inc.
Izod Impact, Unnotched 3.70 J/cm
6.93 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE  (discontinued **)
Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.- Natural: Ixef 5002/008..
Izod Impact, Unnotched 3.70 - 3.70 J/cm

@Temperature -40.0 - -40.0 °C
6.93 - 6.93 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 3.70 J/cm Grade Count:2
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Copyright © lookpolymers.com All Rights Reserved