Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 62.1 - 125 MPa | 9000 - 18100 psi | Average value: 99.3 MPa Grade Count:63 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Tensile Strength, Yield | 26.2001 - 125 MPa @Temperature -40.0 - 120 °C |
3800.01 - 18100 psi @Temperature -40.0 - 248 °F |
Average value: 74.9 MPa Grade Count:2 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Tensile Strength, Yield | 58.6 - 125 MPa | 8500 - 18100 psi | Average value: 88.7 MPa Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Tensile Strength, Yield | 40.5 - 125 MPa | 5870 - 18100 psi | Average value: 89.3 MPa Grade Count:61 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |