Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 - 48.0 MPa
4930 - 6960 psi
ASTM D638
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Tensile Strength, Yield 35.0 - 48.0 MPa
5080 - 6960 psi
ASTM D638
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Tensile Strength, Yield 48.0 - 48.0 MPa

@Temperature 100 - 100 °C
6960 - 6960 psi

@Temperature 212 - 212 °F
Average value: 48.0 MPa Grade Count:1
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..