Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.10 - 12.5 GPa | 450 - 1810 ksi | Average value: 7.42 GPa Grade Count:113 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 2.97 - 12.5 GPa @Temperature -40.0 - 121 °C |
431 - 1810 ksi @Temperature -40.0 - 250 °F |
Average value: 5.07 GPa Grade Count:10 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Flexural Modulus | 5.00 - 12.5 GPa | 725 - 1810 ksi | Average value: 8.93 GPa Grade Count:22 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Modulus | 2.80 - 12.5 GPa | 406 - 1810 ksi | Average value: 7.10 GPa Grade Count:153 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |