Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 5.76 - 13.7 J @Temperature -20.0 - -20.0 °C |
4.25 - 10.1 ft-lb @Temperature -4.00 - -4.00 °F |
Average value: 9.73 J Grade Count:1 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Dart Drop, Total Energy | 5.76 - 13.7 J @Thickness 3.18 - 3.18 mm |
4.25 - 10.1 ft-lb @Thickness 0.125 - 0.125 in |
Average value: 9.73 J Grade Count:1 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |