Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0404 - 1.56 g/cc | 0.00146 - 0.0564 lb/in³ | Average value: 0.683 g/cc Grade Count:39 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Density | 0.700 - 1.56 g/cc | 0.0253 - 0.0564 lb/in³ | Average value: 1.43 g/cc Grade Count:19 |
Overview of materials for Chlorinated PVC (CPVC) This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 1.25 - 1.56 g/cc | 0.0452 - 0.0564 lb/in³ | Average value: 1.41 g/cc Grade Count:23 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1184 |
Fainplast Compounds RH 325 Rigid PVC, Antishock Extrusion Antishock furniture profiles |
|||
Density | 1.44 - 1.56 g/cc | 0.0520 - 0.0564 lb/in³ | Apparent |
Gouda Vuurvast FI 35-15 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 1.44 - 1.56 g/cc | 0.0520 - 0.0564 lb/in³ | Apparent |
Gouda Vuurvast GI 34 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 1.53 - 1.56 g/cc | 0.0553 - 0.0564 lb/in³ | Laminate |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Fabric Form Fiber: T300-3KInformation provided by HexCel |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 0135 Flexible PVC, Flame Retardant Sheathing Sheathing coaxial cables |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 80 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 87/1 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 89/2 Flexible PVC, Flame Retardant Sheathing Operating temperature 75°C |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 80 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 87 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 4522 Halogen Free PVC High flame retardancy |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 95/1 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 87/4 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 215 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flame retardancy, improved processabilityInformation provided by Fainplast Compound.. |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 220 Rigid PVC, Extrusion Various profiles |
|||
Density | 1.53 - 1.56 g/cc | 0.0553 - 0.0564 lb/in³ | Laminate |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |
|||
Density | 1.10 - 1.56 g/cc | 0.0397 - 0.0564 lb/in³ | Average value: 1.24 g/cc Grade Count:177 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1184 |
Fainplast Compounds R 314 Rigid PVC, Extrusion Electric channels and various profiles |
|||
Density | 1.09 - 1.56 g/cc | 0.0394 - 0.0564 lb/in³ | Average value: 1.22 g/cc Grade Count:149 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |