Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000300 - 0.0200 cm/cm
0.000300 - 0.0200 in/in
Average value: 0.00890 cm/cm Grade Count:21
Overview of materials for Polyphthalamide (PPA), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage 0.000300 - 0.0100 cm/cm
0.000300 - 0.0100 in/in
Average value: 0.00539 cm/cm Grade Count:11
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..
Linear Mold Shrinkage 0.000300 - 0.0150 cm/cm
0.000300 - 0.0150 in/in
Average value: 0.00402 cm/cm Grade Count:139
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Linear Mold Shrinkage 0.000300 - 0.0350 cm/cm
0.000300 - 0.0350 in/in
Average value: 0.00391 cm/cm Grade Count:183
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Linear Mold Shrinkage 0.000300 - 0.0200 cm/cm
0.000300 - 0.0200 in/in
Average value: 0.00496 cm/cm Grade Count:111
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage 0.000300 - 0.0350 cm/cm
0.000300 - 0.0350 in/in
Average value: 0.00417 cm/cm Grade Count:497
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..
Linear Mold Shrinkage 0.000300 - 0.00700 cm/cm
0.000300 - 0.00700 in/in
Average value: 0.00163 cm/cm Grade Count:32
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..
Linear Mold Shrinkage 0.000300 - 0.0350 cm/cm
0.000300 - 0.0350 in/in
Average value: 0.00325 cm/cm Grade Count:111
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Linear Mold Shrinkage 0.000300 - 0.00780 cm/cm
0.000300 - 0.00780 in/in
Average value: 0.00304 cm/cm Grade Count:17
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..