Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+13 - 3.00e+16 ohm-cm | 1.00e+13 - 3.00e+16 ohm-cm | Average value: 8.06e+15 ohm-cm Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Electrical Resistivity | 1.00e+12 - 3.00e+16 ohm-cm | 1.00e+12 - 3.00e+16 ohm-cm | Average value: 1.14e+16 ohm-cm Grade Count:14 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Electrical Resistivity | 1000 - 3.00e+16 ohm-cm | 1000 - 3.00e+16 ohm-cm | Average value: 7.45e+15 ohm-cm Grade Count:11 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Electrical Resistivity | 1.00e+15 - 3.00e+16 ohm-cm | 1.00e+15 - 3.00e+16 ohm-cm | Average value: 1.16e+16 ohm-cm Grade Count:7 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Electrical Resistivity | 5.30e+15 - 3.00e+16 ohm-cm | 5.30e+15 - 3.00e+16 ohm-cm | Average value: 2.18e+16 ohm-cm Grade Count:3 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |
|||
Electrical Resistivity | 1.00e+14 - 3.00e+16 ohm-cm | 1.00e+14 - 3.00e+16 ohm-cm | Average value: 1.00e+16 ohm-cm Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Electrical Resistivity | 1000 - 3.00e+16 ohm-cm | 1000 - 3.00e+16 ohm-cm | Average value: 3.87e+15 ohm-cm Grade Count:28 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |
|||
Electrical Resistivity | 1.00e+14 - 3.00e+16 ohm-cm | 1.00e+14 - 3.00e+16 ohm-cm | Average value: 8.08e+15 ohm-cm Grade Count:16 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |