Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 65.0 °C | 149 °F | short period, no load |
Omnia Plastica PVC Polyvinylchloride A widely used material, its application is under regulation in many countries for ecological reasons and it is often substituted by PP or other polymers. It is chosen for its chemical resistance.Fea.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Continuous Use |
Polycasa XT 610 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Acrylic |
Parker Chomerics Tecknit ECTC™ Windows Electrically Conductive Transparent Coating Description: ECTC WINDOWS are custom designed optical display panels produced by depositing a very thin electrically conductive transparent coating directly onto the surface of various optical subst.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | 20,000 hr; IEC 216 |
Nilit Nilamid A3 H ZC High Impact PA66 Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | 20,000 hr; IEC 216 |
Nilit Nilamid A3 H ZE High Impact PA66 Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
Ineos H20Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
BP Amoco Amoco® 7644 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property .. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
BP Amoco Amoco® 7942 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Excellent mold release, AntistaticTypical applications: Closures, Thin-walled rigid packagingComplies with FDA specification, Title 21, CFR .. |
|||
Maximum Service Temperature, Air | 65.0 - 180 °C | 149 - 356 °F | Average value: 129 °C Grade Count:18 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | |
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Pressed Bushings |
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: .. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | |
Zotefoams Evazote® EV30 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Wet Service |
Chesterton ARC 855 Abrasion Control Liquid Description: An advanced ceramic composite formulated to protect equipment from aggressive chemical attack, corrosion, and erosion. The product is a low viscosity composite that is easily applied by.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Deflection Temp at unknown load |
Abatron AboCast 8503-4/AboCure 8503-4 Colorless Epoxy AboCast 8503-4/AboCure 8503-4 is a general purpose, moderate speed, colorless epoxy casting compound with low viscosity. It offers a convenient 2/1 ratio by volume and lends itself to casting of thi.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Long term |
3M 415 Splicing Tape 3M™ Splicing Tapes utilize an acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Short term |
3M 9420 Splicing Tapes 3M™ Splicing Tapes utilize on acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Short term |
3M 9925XL Extended Liner Tapes 3M™ Extended Liner Tapes have a liner that extends beyond the width of the adhesive to provide easy liner starting and removal. The liners, with the exception of 3M™ Extended Liner Tape 450EK is p.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Long Term |
3M XG2105 Hi-Performance Adhesive Transfer Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Short Term |
3M XT2105 Hi-Tack Adhesive Transfer Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Short Term |
3M XT2105-AGT Hi-Tack Adhesive Transfer Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Long Term |
3M XT6110 Hi-Tack Double Coated Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Long term |
3M 401M Double Coated Paper Tapes 3M™ Double Coated Paper Tapes 401M and 410M utilize a natural rubber adhesive system that offers good to excellent adhesion to many types of surfacesInformation provided by 3M |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | Long term |
3M 410M Double Coated Paper Tapes 3M™ Double Coated Paper Tapes 401M and 410M utilize a natural rubber adhesive system that offers good to excellent adhesion to many types of surfacesInformation provided by 3M |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | |
GEHR Plastics ECOGEHR® C-L Cellulose-Lignin Compound
(discontinued **) C-L is comprised of the wood components cellulose, natural fibers, lignin and fatty acids. It possesses many interesting properties that together are very similar to the natural wood. Consequently,.. |
|||
Maximum Service Temperature, Air | 65.0 - 180 °C | 149 - 356 °F | Average value: 98.9 °C Grade Count:10 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
Ineos H35Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Maximum Service Temperature, Air | 65.0 - 70.0 °C | 149 - 158 °F | |
Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLong pot lifeLarge cas.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
Ineos H05Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Closures, DispensersComplies with FDA specification, Title 21, CFR 177.1520.Typical property data.. |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
BP Amoco Amoco® Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection molding; Rotary CompressionFeatures: Nucleated, Antistatic, LubricatedTypical applications: Closures, CapsComplies with FDA specification, Title 21, CFR 177... |
|||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | UL Relative Thermal Index |
Ineos H35G-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520... |