Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.427 - 7.52 J/cm | 0.800 - 14.1 ft-lb/in | Average value: 1.32 J/cm Grade Count:112 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |