Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.50 - 8.50 J/cm² | 7.14 - 40.5 ft-lb/in² | Average value: 4.01 J/cm² Grade Count:22 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 1.50 - 2.00 J/cm² @Temperature -40.0 - -20.0 °C |
7.14 - 9.52 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.77 J/cm² Grade Count:2 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact Unnotched | >= 1.50 J/cm² @Temperature 23.0 °C |
>= 7.14 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
Qualchem Danamid FGFS-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Impact modified.Information provided by Qualchem Zrt. |
|||
Charpy Impact Unnotched | 1.50 - 1000 J/cm² | 7.14 - 4760 ft-lb/in² | Average value: 1.50 J/cm² Grade Count:3 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² - NB | 7.14 ft-lb/in² - NB | Average value: 9.27 J/cm² Grade Count:116 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Charpy Impact Unnotched | 1.50 - 10.0 J/cm² | 7.14 - 47.6 ft-lb/in² | Average value: 5.14 J/cm² Grade Count:58 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact Unnotched | 1.50 - 1.50 J/cm² @Temperature -20.0 - -20.0 °C |
7.14 - 7.14 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 1.50 J/cm² Grade Count:1 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² - NB | 7.14 ft-lb/in² - NB | Average value: 7.98 J/cm² Grade Count:42 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-7687 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
LATI Laril 13-V1KC PPOm, Mineral Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Mineral filler. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good therm.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
LATI Latimass 82-02 D030 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179 |
Styrolution PS ESCRimo HIPS Styrolution PS ESCRimo is a high impact polystyrene grade with an improved stress cracking resistance compared to conventional high impact polystyreneHigh ESCR resistanceDeep draw thermoformingUL 94.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179/1eU |
Polyplastics TOPAS® 6013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Due to its high transparency, low levels of eluates, superior chemical resistance, and high heat deflection temperature, this grade is suitable for products such as pharmaceutical packaging and diag.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179/1eU |
Polyplastics TOPAS® 6015 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) A similar grade to 6013. However, heat deflection temperature is (HDT/B) = 150°C. This is a temperature that cannot be achieved with many other amorphous polymers.Information provided by PolyPlasti.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BGM-65 X V0 PA6-(GF+MD)65 Product description: Grilon BGM-65 X V0 is a flame retardant mineral and glass fiber reinforced PA6 injection molding grade. Grilon BGM-65 X V0 has the following important properties: Halogen and ph.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3340 PC Polypropylene Nucleated grade for injection moldings with higher transparency.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature 5.00 °C |
7.14 ft-lb/in² @Temperature 41.0 °F |
ISO 179 |
BASF Petra® 7010 WT 7729 15% Glass Filled PET Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface .. |
|||
Charpy Impact Unnotched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® D 1133 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
BASF Procom® T40H 550 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.50 J/cm² - NB @Temperature -30.0 - -20.0 °C |
7.14 ft-lb/in² - NB @Temperature -22.0 - -4.00 °F |
Average value: 5.64 J/cm² Grade Count:42 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Charpy Impact Unnotched | 1.50 - 4.50 J/cm² | 7.14 - 21.4 ft-lb/in² | Average value: 3.37 J/cm² Grade Count:7 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | |
LATI Latimass 62-01 D025 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Charpy Impact Unnotched | 1.50 J/cm² | 7.14 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Charpy Impact Unnotched | 1.50 - 999.9 J/cm² @Temperature -20.0 - -20.0 °C |
7.14 - 4759 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 5.63 J/cm² Grade Count:9 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |