Polymer Property : Flexural Modulus = 1650.03 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.44022 - 11.3763 GPa

@Temperature -40.0 - 121 °C
644.010 - 1650.03 ksi

@Temperature -40.0 - 250 °F
Average value: 6.48 GPa Grade Count:13
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..