Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 152 - 166 °C | 305 - 331 °F | Average value: 161 °C Grade Count:5 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 127 - 166 °C | 260 - 331 °F | Average value: 150 °C Grade Count:26 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 120 - 166 °C | 248 - 331 °F | Average value: 158 °C Grade Count:80 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 132 - 166 °C | 270 - 330 °F | Average value: 143 °C Grade Count:5 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |