Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.67 - 9.08 J/cm
5.00 - 17.0 ft-lb/in
Average value: 6.11 J/cm Grade Count:25
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Unnotched 2.67 - 9.08 J/cm
5.00 - 17.0 ft-lb/in
Average value: 6.12 J/cm Grade Count:57
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Izod Impact, Unnotched 8.00 - 9.10 J/cm
15.0 - 17.0 ft-lb/in
Average value: 8.53 J/cm Grade Count:3
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported ..
Izod Impact, Unnotched 6.90 - 9.10 J/cm
12.9 - 17.0 ft-lb/in
Average value: 7.77 J/cm Grade Count:3
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Izod Impact, Unnotched 5.34 - 9.08 J/cm
10.0 - 17.0 ft-lb/in
Average value: 6.80 J/cm Grade Count:14
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Izod Impact, Unnotched 0.427 - 9.08 J/cm
0.800 - 17.0 ft-lb/in
Average value: 5.03 J/cm Grade Count:32
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Izod Impact, Unnotched 1.39 - 9.08 J/cm
2.60 - 17.0 ft-lb/in
Average value: 2.95 J/cm Grade Count:33
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Izod Impact, Unnotched 1.49 - 9.08 J/cm
2.79 - 17.0 ft-lb/in
Average value: 5.61 J/cm Grade Count:42
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Copyright © lookpolymers.com All Rights Reserved