Polymer Property : Dielectric Strength = 19.7 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 19.7 - 41.0 kV/mm
500 - 1040 kV/in
Average value: 27.1 kV/mm Grade Count:3
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Dielectric Strength 19.7 kV/mm
500 kV/in
Short Term; in air; ASTM D 149
RTP Company RTP 800 Acetal (POM), Base Resin
Dielectric Strength 19.7 kV/mm

@Thickness 3.17 mm
500 kV/in

@Thickness 0.125 in
Ineos Nova 1230 High Heat Crystal Polystyrene  (discontinued **)
Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r..
Dielectric Strength 19.7 kV/mm

@Thickness 3.17 mm
500 kV/in

@Thickness 0.125 in
Ineos Nova 1531 High Heat Crystal Polystyrene  (discontinued **)
High flow and high heat resistance, Excellent clarityApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical p..
Dielectric Strength 19.7 - 23.0 kV/mm
500 - 584 kV/in
Average value: 20.8 kV/mm Grade Count:3
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Dielectric Strength 19.7 kV/mm
500 kV/in
S/T; ASTM D149
RTP Company RTP 200D TFE 20 SI 2.5  Nylon 6/12 (PA 6/12) PTFE 20% - Silicone 2.5%  (disconti
PTFE 20% - Silicone 2.5%Comments:LubricatedSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provid..
Dielectric Strength 19.7 kV/mm

@Thickness 3.17 mm
500 kV/in

@Thickness 0.125 in
Ineos Nova 1300 High Heat Crystal Polystyrene
High heat resistance, High strength, Good processing characteristics, USP Class ViApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation..
Dielectric Strength 19.7 kV/mm

@Thickness 3.17 mm
500 kV/in

@Thickness 0.125 in
Ineos Nova 5410 High Impact Polystyrene
High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverages cups, Custom sheetProperties were determined on injection molded specimens at 23°C ..
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® ASA GF15 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites..
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PA6 GF/B20 A3 BK 20% Glass Fiber/Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: ..
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PA6 GF6 UG BK MB 6% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance..
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PA6/6 GF33 LE 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Extraction ResistantProcessing Method: Injection MoldingInformation provided b..
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PA6/6 GF40 L 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p..
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PA6/6 GF55 HS L BK 55% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu..
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Luriblend® PA6 TL10 Nylon 6
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (10%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Dielectric Strength 19.7 kV/mm
500 kV/in
Saint-Gobain COHRlastic® Furo 407 Thermally Conductive Silicone Coated Fabric
Description: Conductive silicones expand the use of our products into the electronic assembly market. By the use of special fillers, silicone can be made thermally or electrically conductive. Furo 4..
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Luriblend® PA6/6 GF30 ML5 HS BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and He..
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Luriblend® PPS GF30 TL15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Dielectric Strength 19.7 kV/mm
500 kV/in
ASTM D 696
Styrolution PS 2610 GPPS
Extruded packaging; Thermoforming applicationsExcellent toughnessHigh melt strengthGood flow and processabilityInformation provided by Styrolution
Dielectric Strength 19.7 kV/mm
500 kV/in
Short Term; in oil; ASTM D 149
RTP Company RTP 201 FR Nylon 6/6 (PA), Glass Fiber - Flame Retardant - UL94 V-0
The RTP series of flame retardant, glass fiber reinforced nylon materials are designed to provide the optimal balance of strength, electrical and ignition resistance properties while exhibiting exce..
Dielectric Strength 19.7 kV/mm
500 kV/in
Short Term; in oil; ASTM D 149
RTP Company RTP 201 FR UV Nylon 6/6 (PA), Glass Fiber - Flame Retardant - UV Stabilized - UL94 V-0
The RTP series of flame retardant, glass fiber reinforced nylon materials are designed to provide the optimal balance of strength, electrical and ignition resistance properties while exhibiting exce..
Dielectric Strength 19.7 kV/mm
500 kV/in
Short Term; in oil; ASTM D 149
RTP Company RTP 2101 Polyetherimide (PEI), Glass Fiber
Dielectric Strength 19.7 kV/mm
500 kV/in
3M HDT Heat Shrink Tubing
3M Heat Shrink Tubing HDT is a designed to provide reliable performance as well as excellent mechanical and environmental protection. This flame-retardant product combines the important advantage of..
Dielectric Strength 19.7 kV/mm
500 kV/in
Arkema Group Altuglas® GR 7E LIL Acrylic
ALTUGLAS GR 7E LIL is an injection molding grade with excellent balance between mechanical, thermal and optical properties.Key features : easy processing and demolding improved chemical resistance ..
Dielectric Strength 19.7 kV/mm
500 kV/in
S/T; ASTM D149
RTP Company RTP 200C  Nylon 11 (PA 11) Base Resin  (discontinued **)
Base ResinComments:UnfilledUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this pro..
Dielectric Strength 19.7 kV/mm
500 kV/in
S/T; ASTM D149
RTP Company RTP 201D  Nylon 6/12 (PA 6/12) Glass Fiber 10%  (discontinued **)
Glass Fiber 10%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Dielectric Strength 19.7 kV/mm
500 kV/in
Arkema Group Oroglas® V 045 Acrylic, Extrusion Grade  (discontinued **)
OROGLAS V 045 is a lubricated extrusion grade offering good combination of physical and optical properties.OROGLAS V 045 provides easy processing behavior.OROGLAS V 045 is recommended for extrusion..
Dielectric Strength 19.7 kV/mm
500 kV/in
Arkema Group Oroglas® V 045 I Acrylic, Extrusion Grade  (discontinued **)
OROGLAS V 045 I is an extrusion that exhibits the following properties : 50% tougher than standard acrylics excellent optical properties ( comparable to that of standard acrylics) superior surface ..
Dielectric Strength 19.7 kV/mm
500 kV/in
Ineos Nova 204L Crystal Polystyrene General Purpose Grade  (discontinued **)
Fast cycling, Good heat resistance, Good balance of properties and flow characteristics, Extrusion and Injection Molding Applications: General purpose injection molded itemsProperties were determin..
Dielectric Strength 19.7 kV/mm
500 kV/in
Short Term; in oil; ASTM D 149
RTP Company RTP 1003 FR A Polybutylene Terephthalate (PBT), Glass Fiber - Flame Retardant - UL94 V-0
RTP 1001 - 1005 FRA are a series of glass fiber reinforced, flame retardant PBT compounds. All are UL94 V-0 certified down to the 1/32" (0.8mm) thickness. These materials exhibit easy flow, excellen..