Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 60.0 - 175.816 MPa @Temperature -40.0 - 93.3 °C |
8700 - 25500.0 psi @Temperature -40.0 - 200 °F |
Average value: 80.8 MPa Grade Count:16 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |