Polymer Property : Charpy Impact, Notched = 4.50 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.160 - 4.50 J/cm²
0.761 - 21.4 ft-lb/in²
Average value: 0.723 J/cm² Grade Count:35
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Charpy Impact, Notched 0.400 - 4.50 J/cm²
1.90 - 21.4 ft-lb/in²
Average value: 1.23 J/cm² Grade Count:39
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Charpy Impact, Notched 0.400 - 4.50 J/cm²
1.90 - 21.4 ft-lb/in²
Average value: 2.03 J/cm² Grade Count:34
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Charpy Impact, Notched 0.300 - 4.50 J/cm²

@Temperature -30.0 - 30.0 °C
1.43 - 21.4 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.92 J/cm² Grade Count:25
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Charpy Impact, Notched 1.10 - 4.50 J/cm²

@Temperature -30.0 - 30.0 °C
5.24 - 21.4 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 3.03 J/cm² Grade Count:8
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Charpy Impact, Notched 0.350 - 4.50 J/cm²

@Temperature -40.0 - 30.0 °C
1.67 - 21.4 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 1.39 J/cm² Grade Count:39
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Charpy Impact, Notched 3.50 - 4.50 J/cm²
16.7 - 21.4 ft-lb/in²
DIN 53453
Zell-Metall Engineering Plastics Zellamid 1115
By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads ..
Charpy Impact, Notched 2.00 - 4.50 J/cm²
9.52 - 21.4 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound
UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit..
Charpy Impact, Notched 0.300 - 4.50 J/cm²
1.43 - 21.4 ft-lb/in²
Average value: 2.14 J/cm² Grade Count:42
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..