Electrical Properties Metric English Comments
Dielectric Strength 20.0 - 25.0 kV/mm
508 - 635 kV/in
IEC 60243-1
Raschig Group MELOPAS® 6605 MP Melamine
Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be..
Dielectric Strength 20.0 - 25.0 kV/mm
508 - 635 kV/in
IEC 60243-1
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
Dielectric Strength 20.0 - 25.0 kV/mm
508 - 635 kV/in
IEC 60243-1
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
Dielectric Strength 24.0 - 25.0 kV/mm
610 - 635 kV/in
Average value: 24.3 kV/mm Grade Count:3
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Dielectric Strength 16.7 - 25.0 kV/mm
425 - 635 kV/in
Average value: 19.6 kV/mm Grade Count:7
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
508 - 635 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
ASTM D149
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers.
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
508 - 635 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
ASTM D149
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
508 - 635 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
ASTM D149
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers.
Dielectric Strength 7.00 - 25.0 kV/mm
178 - 635 kV/in
Average value: 11.2 kV/mm Grade Count:7
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi..
Dielectric Strength 11.0 - 25.0 kV/mm
279 - 635 kV/in
Average value: 21.0 kV/mm Grade Count:7
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
Dielectric Strength 15.7 - 25.0 kV/mm
400 - 635 kV/in
Average value: 19.6 kV/mm Grade Count:6
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v..
Dielectric Strength 20.0 - 25.0 kV/mm
508 - 635 kV/in
ASTM D149
Isoflon PTFE + 15% Ceramic Polytetrafluoroethylene with 15% Ceramic
Properties:Improved compression resistanceGood dielectric characteristicsGood thermal insulationMachining can be trickyApplications: Electrical applicationsInformation provided by Isoflon.
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm
508 - 635 kV/in

@Thickness 0.0394 in
ASTM D149
Solvay Specialty Polymers Ajediumâ„¢ PVDF 9009 Polyvinylidene Fluoride (PVDF)
Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea..
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm
508 - 635 kV/in

@Thickness 0.0394 in
ASTM D149
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF)
Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope..
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm
508 - 635 kV/in

@Thickness 0.0394 in
ASTM D149
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal..
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm
508 - 635 kV/in

@Thickness 0.0394 in
ASTM D149
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm
508 - 635 kV/in

@Thickness 0.0394 in
ASTM D149
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF)
Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm
508 - 635 kV/in

@Thickness 0.0394 in
ASTM D149
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D..
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm
508 - 635 kV/in

@Thickness 0.0394 in
ASTM D149
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6..
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm
508 - 635 kV/in

@Thickness 0.0394 in
ASTM D149
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)
Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat..
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm
508 - 635 kV/in

@Thickness 0.0394 in
ASTM D149
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53...
Dielectric Strength 15.0 - 25.0 kV/mm
381 - 635 kV/in
DC Breakdown Strength
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain)
LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good ..
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
508 - 635 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
ASTM D149
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
508 - 635 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
ASTM D149
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers.
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
508 - 635 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
ASTM D149
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Dielectric Strength 20.0 - 25.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
508 - 635 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
ASTM D149
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)  (discontinued **)
Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Dielectric Strength 16.0 - 25.0 kV/mm
406 - 635 kV/in
DIN 53481
Isoflon PA 6 Polyamide 6
General use for mechanical partsGood heat resistanceEasy to useHigh moisture regainInformation provided by Isoflon.
Dielectric Strength 23.0 - 25.0 kV/mm
584 - 635 kV/in
DIN 53481
Isoflon PAI Polyamideimide
Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon.
Dielectric Strength 19.7 - 25.0 kV/mm
500 - 635 kV/in
Average value: 21.1 kV/mm Grade Count:11
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Dielectric Strength 2.60 - 25.0 kV/mm
66.0 - 635 kV/in
Average value: 23.1 kV/mm Grade Count:51
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..
Copyright © lookpolymers.com All Rights Reserved