Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 1.50 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.50 J/cm²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Nilit FRIANYL B63 CU90 Nylon 6.6 for injection molding, 90% copper filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 KF50 Nylon 6 for injection molding, 50% short glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.50 - 1.80 J/cm²
7.14 - 8.57 ft-lb/in²
Injection and Compression; ISO 179/1eU
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel..
Charpy Impact Unnotched 1.50 - 8.50 J/cm²
7.14 - 40.5 ft-lb/in²
Average value: 4.01 J/cm² Grade Count:22
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C4220 is a 20% glass reinforced, non FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance that combines a good processabity with a lo..
Charpy Impact Unnotched >= 1.50 J/cm²

@Temperature 23.0 °C
>= 7.14 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Qualchem Danamid FGFS-30 Polyamide 6, 30% Glass Fiber
Reinforced with glass fiber. Impact modified.Information provided by Qualchem Zrt.
Charpy Impact Unnotched 1.50 J/cm² - NB
7.14 ft-lb/in² - NB
Average value: 4.92 J/cm² Grade Count:68
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eU
Celanese VECTRA B230 LCP, 30% Specialty  (Unverified Data**)
Exceptional strength and stiffness. Suitable for metal replacement applications. Electrically conductive. 30% carbon fiber reinforced.30% carbon fiber,exceptional strength and stiffness, conductiv..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15/BK PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1700-7910 PPO, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 80-8222 Polyacetal-copolymer, with mineral filler, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
LATI Latigea B01 L/07 Bio-Polymer
Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
LATI Latigray 80-03 CWG/850 PPS, Glass/Metallic Reinforced
Radiopaque compound based on Polyphenylene Sulfide (PPS). Metallic filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
LATI Latigray 82-04 CX/90 PA 12
Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
LATI Latimass 82-02 D030 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eU
Polyplastics TOPAS® 6013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade)
Due to its high transparency, low levels of eluates, superior chemical resistance, and high heat deflection temperature, this grade is suitable for products such as pharmaceutical packaging and diag..
Charpy Impact Unnotched 1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1fU
Evonik Corporation Plexiglas® 99560 Superclear Extruded PMMA Sheet
Description: PLEXIGLAS® Superclear 99560 is an extruded PMMA product that has been developed for applications with highest demands on optical and surface quality. It has no observable haze, a very ..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
Evonik Corporation Vestyron® 224 Polystyrene
Uses: Packaging made from thermoforming sheets blended with high impact polystyrene panels.ISO data as provided by the manufacturer.
Charpy Impact Unnotched 1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® BGM-65 X V0 PA6-(GF+MD)65
Product description: Grilon BGM-65 X V0 is a flame retardant mineral and glass fiber reinforced PA6 injection molding grade. Grilon BGM-65 X V0 has the following important properties: Halogen and ph..
Charpy Impact Unnotched 1.50 J/cm²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 3340 PC Polypropylene
Nucleated grade for injection moldings with higher transparency.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.50 J/cm²

@Temperature 5.00 °C
7.14 ft-lb/in²

@Temperature 41.0 °F
ISO 179
BASF Petra® 7010 WT 7729 15% Glass Filled PET
Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface ..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eU
Celanese VECTRA B230 LCP, 30% Specialty
Exceptional strength and stiffness. Suitable for metal replacement applications. Electrically conductive. 30% carbon fiber reinforced.Information provided by Celanese
Charpy Impact Unnotched >= 1.50 J/cm²
>= 7.14 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR N 4111 Bulk Molding Compound
Smooth, high gloss surface. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion..
Charpy Impact Unnotched 1.50 J/cm²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1102 M Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.50 J/cm²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
BASF Procom® D 1133 Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eU
Celanese VECTRA A700 LCP, 30% Specialty
Some conductivity. Suitable for electrostatic dissipation (ESD) applications. 30% glass reinforced.Information provided by Celanese
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
LATI Latigray 82-05 CX/90 PA 12
Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301-8305 PPS, linear, with glass fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam..
Charpy Impact Unnotched 1.50 J/cm² - NB

@Temperature -40.0 - 30.0 °C
7.14 ft-lb/in² - NB

@Temperature -40.0 - 86.0 °F
Average value: 4.74 J/cm² Grade Count:124
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..