Polymer Property : Maximum Service Temperature, Air = 284 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 85.0 - 140 °C
185 - 284 °F
Average value: 109 °C Grade Count:7
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
Average value: 128 °C Grade Count:5
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Maximum Service Temperature, Air 130 - 140 °C
266 - 284 °F
Heat distortion temperature
Abatron AboCast 8101-1/AboCure 8101-1 Epoxy  (discontinued **)
Data provided by the manufacturer, Abatron, Inc. Medium-viscosity, Light Amber color. Shelf life is 12+ months.Corrosion Resistance Best Abatron "VR" Epoxy for heat, solvent and chemical resistanc..
Maximum Service Temperature, Air 130 - 140 °C
266 - 284 °F
Heat distortion temperature
Abatron AboCast 8101-2/AboCure 8101-2 Epoxy  (discontinued **)
Data provided by the manufacturer, Abatron, Inc. Lower-viscosity than AboCast 8101-1 for easier casting, encapsulating and potting. Shelf life is 12+ months.Processing: 2-1 ratio. Pot life: 2-3 hr..
Maximum Service Temperature, Air 130 - 140 °C
266 - 284 °F
Heat distortion temperature
Abatron AboWeld 8101-6/AboCure 8101-6 Epoxy  (discontinued **)
Data provided by the manufacturer, Abatron, Inc. Vaseline like consistency, Light Amber color. Similar to AboCast 55-22. Best Abatron "VR" Epoxy for thermal, chemical, and solvent resistance. She..
Maximum Service Temperature, Air 130 - 140 °C
266 - 284 °F
Heat distortion temperature
Abatron AboWeld 8101-7/AboCure 8101-7 Epoxy  (discontinued **)
Data provided by the manufacturer, Abatron, Inc. Paste form, Modified for minimum shrinkage and maximum heat transfer. Similar to 55-25, but better rigidity, hardness, heat and chemical resistance...
Maximum Service Temperature, Air 130 - 140 °C
266 - 284 °F
Heat distortion temperature
Abatron AboWeld 8101-9/AboCure 8101-9 Epoxy  (discontinued **)
Data provided by the manufacturer, Abatron, Inc. Aluminum filled thixotropic paste. Highest heat, solvent and chemical resistance. Shelf life is 12+ months.Processing: Pot life: 1-2 hrs. 2/1 ratio..
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
medium time operation
Zell-Metall Engineering Plastics Zellamid 1100
Zellamid® 1100 is the registered trademark for Zell-Metall’s cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers ..
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
medium time operation
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH
Zellamid® 1100 is the registered trademark for Zell-Metall’s cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers ..
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
medium time operation
Zell-Metall Engineering Plastics Zellamid 1100 MO
Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
medium time operation
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH
Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
medium time operation
Zell-Metall Engineering Plastics Zellamid 1100 OIL
Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces ..
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
medium time operation
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH
Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces ..
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
medium time operation
Zell-Metall Engineering Plastics Zellamid 1115
By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads ..
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
medium time operation
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH
By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads ..
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
long term; EMS
EMS-Grivory Grivory® XE 4071 black 9992 PA612
Product description: Grilamid XE 4071 BLACK 9992 is an impact modified unreinforced high viscosity polyamide 612 (PA612) extrusion grade with superior heat and hydrolysis resistance. Compared to sta..
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
long term; EMS
EMS-Grivory Grivory® XE 4071 nat PA612-I
Product description: Grilamid XE 4071 NATURAL is an unreinforced impact modified high viscosity polyamide 612 (PA612) extrusion grade with superior hydrolysis and heat resistance. Compared to standa..
Maximum Service Temperature, Air 120 - 140 °C
248 - 284 °F
long term; EMS
EMS-Grivory Grivory® BG-50 H PA6-GF50
Product description: Grilon BG-50 H is a high heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 H has the following important properties: High stiffnessHigh heat resist..
Maximum Service Temperature, Air 90.0 - 140 °C
194 - 284 °F
long term; EMS
EMS-Grivory Grivory® BG-50 S PA6-GF50
Product description: Grilon BG-50 S is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 S has the following important properties: High stiffnessExcellent surface fin..
Maximum Service Temperature, Air 130 - 140 °C
266 - 284 °F
Average value: 133 °C Grade Count:3
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..
Maximum Service Temperature, Air 75.0 - 140 °C
167 - 284 °F
Average value: 115 °C Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Maximum Service Temperature, Air 65.0 - 140 °C
149 - 284 °F
Average value: 104 °C Grade Count:7
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
Maximum Service Temperature, Air 65.0 - 140 °C
149 - 284 °F
Average value: 113 °C Grade Count:3
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Maximum Service Temperature, Air 90.0 - 140 °C
194 - 284 °F
Average value: 116 °C Grade Count:3
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..
Maximum Service Temperature, Air 75.0 - 140 °C
167 - 284 °F
Average value: 111 °C Grade Count:11
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..