Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.34 - 2.26 g/cc
0.0484 - 0.0816 lb/in³
Average value: 1.67 g/cc Grade Count:14
Water Absorption 0.0200 - 0.0500 %
0.0200 - 0.0500 %
Average value: 0.0371 % Grade Count:7
Linear Mold Shrinkage 0.00200 - 0.0100 cm/cm
0.00200 - 0.0100 in/in
Average value: 0.00671 cm/cm Grade Count:7
Melt Flow 75.0 - 5000 g/10 min
75.0 - 5000 g/10 min
Average value: 1040 g/10 min Grade Count:15
Ash 0.400 - 0.800 %
0.400 - 0.800 %
Average value: 0.600 % Grade Count:10
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93.0 - 100
93.0 - 100
Average value: 96.3 Grade Count:3
Tensile Strength, Ultimate 27.6 - 150 MPa
4000 - 21800 psi
Average value: 84.3 MPa Grade Count:10
Elongation at Break 0.700 - 30.0 %
0.700 - 30.0 %
Average value: 5.07 % Grade Count:9
Modulus of Elasticity 3.40 - 17.2 GPa
493 - 2500 ksi
Average value: 8.40 GPa Grade Count:6
Flexural Yield Strength 51.7 - 230 MPa
7500 - 33400 psi
Average value: 142 MPa Grade Count:14
Flexural Modulus 3.10 - 21.0 GPa
450 - 3050 ksi
Average value: 9.79 GPa Grade Count:13
Izod Impact, Notched 0.400 - 0.801 J/cm
0.749 - 1.50 ft-lb/in
Average value: 0.586 J/cm Grade Count:6
Izod Impact, Unnotched 0.534 - 13.0 J/cm
1.00 - 24.4 ft-lb/in
Average value: 5.23 J/cm Grade Count:6
Izod Impact, Notched (ISO) 4.00 - 7.00 kJ/m²
1.90 - 3.33 ft-lb/in²
Average value: 5.00 kJ/m² Grade Count:3
7.00 - 7.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.00 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.80 - 2.80 J/cm²

@Temperature -30.0 - -30.0 °C
13.3 - 13.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 2.80 J/cm² Grade Count:1
Charpy Impact, Notched 0.700 - 0.700 J/cm²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.700 J/cm² Grade Count:1
Thermal Properties Metric English Comments
CTE, linear 10.0 - 53.0 µm/m-°C
5.56 - 29.4 µin/in-°F
Average value: 31.7 µm/m-°C Grade Count:12
120 - 120 µm/m-°C

@Temperature 100 - 200 °C
66.7 - 66.7 µin/in-°F

@Temperature 212 - 392 °F
Average value: 120 µm/m-°C Grade Count:2
CTE, linear, Transverse to Flow 17.0 - 50.0 µm/m-°C
9.44 - 27.8 µin/in-°F
Average value: 36.3 µm/m-°C Grade Count:6
Thermal Conductivity 0.255 - 0.300 W/m-K
1.77 - 2.08 BTU-in/hr-ft²-°F
Average value: 0.287 W/m-K Grade Count:6
Melting Point 280 - 282 °C
536 - 540 °F
Average value: 281 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 149 - 281 °C
300 - 538 °F
Average value: 206 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 75.0 - 270 °C
167 - 518 °F
Average value: 180 °C Grade Count:10
Glass Transition Temp, Tg 90.0 °C
194 °F
Average value: 90.0 °C Grade Count:3
Flammability, UL94 V-0
V-0
Grade Count:12
Oxygen Index 44.0 - 47.0 %
44.0 - 47.0 %
Average value: 45.0 % Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 - 1.00e+16 ohm-cm
1.00e+15 - 1.00e+16 ohm-cm
Average value: 8.71e+15 ohm-cm Grade Count:7
Surface Resistance 1e+05 - 1.00e+16 ohm
1e+05 - 1.00e+16 ohm
Average value: 7.00e+15 ohm Grade Count:4
1.00e+12 - 1.00e+12 ohm

@Temperature 90.0 - 90.0 °C
1.00e+12 - 1.00e+12 ohm

@Temperature 194 - 194 °F
Average value: 1.00e+12 ohm Grade Count:2
Dielectric Constant 3.10 - 12.0
3.10 - 12.0
Average value: 4.81 Grade Count:11
Dielectric Strength 11.0 - 25.0 kV/mm
279 - 635 kV/in
Average value: 21.0 kV/mm Grade Count:7
Dissipation Factor 0.000900 - 0.0200
0.000900 - 0.0200
Average value: 0.00345 Grade Count:11
Arc Resistance 20.0 - 50.0 sec
20.0 - 50.0 sec
Average value: 40.0 sec Grade Count:3
Processing Properties Metric English Comments
Mold Temperature 135 - 177 °C
275 - 350 °F
Average value: 153 °C Grade Count:3
Injection Pressure 34.5 - 103 MPa
5000 - 15000 psi
Average value: 80.4 MPa Grade Count:3
Users viewing this material also viewed the following: