Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-1000 AS Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | At 8-20% Dosing; ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 5000 Polyolefin Compatible Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 5000 is a polyolefin compatible dissipative masterbatch developed for PP injection moulded products. The active substance is an IDP (inherently dissipative polymer) and it gives a per.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | IEC 60093 |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | IEC 60093 |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | IEC 60093 |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Surface Resistance | 1.00 - 1.00e+12 ohm | 1.00 - 1.00e+12 ohm | Average value: 6.17e+10 ohm Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Surface Resistance | 0.0300 - 1.00e+12 ohm | 0.0300 - 1.00e+12 ohm | Average value: 3.13e+10 ohm Grade Count:21 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Surface Resistance | 1.00 - 1.00e+12 ohm | 1.00 - 1.00e+12 ohm | Average value: 1.44e+10 ohm Grade Count:92 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Surface Resistance | 1000 - 1.00e+12 ohm | 1000 - 1.00e+12 ohm | Average value: 3.33e+11 ohm Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min.. |
|||
Surface Resistance | 1000 - 1.00e+12 ohm | 1000 - 1.00e+12 ohm | Average value: 4.65e+11 ohm Grade Count:11 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
Techmer ES Electrablend® ABS CF5 5% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 5% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 LNP* STAT-LOY* 9X03508 is a compound based on PPO+PA66 resin containing Proprietary Filler(s). Added features of this material include: Antistatic, Flame Retardant, High Impact. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Europe-Africa-Middle East) LNP* Stat-loy* A3000 is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: Antistat. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000TXJ ABS LNP* STAT-LOY* A3000TXJ is a product based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS LNP* STAT-LOY* AF3009 is a compound based on ABS resin containing 10% Glass Fiber. Added features of this material include: Antistatic, Flame Retardant. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS LNP* STAT-LOY* N30009 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
Techmer ES Statiblend® 02056 BKN Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9109116Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
Techmer ES Statiblend® 02056 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9111116Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL NC208 PPE+HIPS (Asia Pacific) |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY KX01002 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX01002 is a compound based on Acetal Copolymer resin containing Antistat. Added features include: Permanent Anti-Static. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY NX03583 PC+ABS LNP STAT-LOY* NX03583 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant. |
|||
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | IS 3396-1979 |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | IS 3396-1979 |
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | Average value: 1.04e+11 ohm Grade Count:11 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | ASTM D257 |
Supreme Petrochem SP 6630 Antistatic Polystyrene Characteristics Easy flow Excellent transparency Processing Extrusion Applications For glossy cap layer on HIPS To prevent dust patterns on thermoformed products Material Status: Commercial : Acti.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® LC108 PC (Asia Pacific) Polycarbonate base, 8% carbon fiber reinforced, FR |