Polymer Property : Charpy Impact, Notched = 3.33 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.400 - 0.700 J/cm²

@Temperature 23.0 °C
1.90 - 3.33 ft-lb/in²

@Temperature 73.4 °F
Injection and Compression; ISO 179/ 1eA
Raschig Group EPOXIDUR® 3582 EP Epoxy
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi..
Charpy Impact, Notched 0.700 - 0.700 J/cm²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.700 J/cm² Grade Count:1
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 0.350 - 0.700 J/cm²

@Temperature -30.0 - -30.0 °C
1.67 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.550 J/cm² Grade Count:10
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Charpy Impact, Notched 0.700 - 0.700 J/cm²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.700 J/cm² Grade Count:2
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Charpy Impact, Notched 0.200 - 0.700 J/cm²

@Temperature -30.0 - -20.0 °C
0.952 - 3.33 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.283 J/cm² Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Charpy Impact, Notched 0.200 - 0.700 J/cm²
0.952 - 3.33 ft-lb/in²
Average value: 0.529 J/cm² Grade Count:12
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Charpy Impact, Notched 0.500 - 0.700 J/cm²
2.38 - 3.33 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Charpy Impact, Notched 0.500 - 0.700 J/cm²

@Temperature 23.0 °C
2.38 - 3.33 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group SURAPLAST UPA 63 UP
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
Charpy Impact, Notched 0.600 - 0.700 J/cm²

@Temperature -20.0 - -20.0 °C
2.86 - 3.33 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.629 J/cm² Grade Count:7
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Charpy Impact, Notched 0.600 - 0.700 J/cm²

@Temperature -20.0 - -20.0 °C
2.86 - 3.33 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.680 J/cm² Grade Count:5
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Charpy Impact, Notched 0.200 - 0.700 J/cm²

@Temperature -30.0 - -20.0 °C
0.952 - 3.33 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.445 J/cm² Grade Count:20
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Charpy Impact, Notched 0.700 - 0.700 J/cm²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.700 J/cm² Grade Count:1
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
Charpy Impact, Notched 0.500 - 0.700 J/cm²
2.38 - 3.33 ft-lb/in²
Average value: 0.600 J/cm² Grade Count:5
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu..
Charpy Impact, Notched 0.200 - 0.700 J/cm²

@Temperature -40.0 - -20.0 °C
0.952 - 3.33 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.391 J/cm² Grade Count:15
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.300 - 0.700 J/cm²

@Temperature -30.0 - -30.0 °C
1.43 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.583 J/cm² Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
Charpy Impact, Notched 0.700 - 0.700 J/cm²

@Temperature -30.0 - -30.0 °C
3.33 - 3.33 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.700 J/cm² Grade Count:1
Overview of materials for Nylon 6, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria..
Charpy Impact, Notched 0.400 - 0.700 J/cm²
1.90 - 3.33 ft-lb/in²
Average value: 0.519 J/cm² Grade Count:7
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.100 - 0.700 J/cm²

@Temperature -20.0 - -20.0 °C
0.476 - 3.33 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.303 J/cm² Grade Count:11
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..