Mechanical Properties Metric English Comments
Modulus of Elasticity 3.40 GPa
493 ksi
ASTM D638
Plaskolite Optix® CA-80 General Purpose Acrylic Resin
Extrusion Grade Pellets. Unlubricated version of CA-81. Highest Molecular weight.
Modulus of Elasticity 3.40 GPa
493 ksi
ASTM D638
Plaskolite Optix® CA-81 General Purpose Acrylic Resin
Extrusion Grade Pellets. Highest Molecular weight.
Modulus of Elasticity 3.40 GPa
493 ksi
dry
Murtfeldt Murylon® HT Nylon 46
The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entir..
Modulus of Elasticity 3.40 GPa
493 ksi
ASTM D638
Plaskolite West Optix® CA-80 General Purpose Acrylic Resin
Extrusion Grade Pellets. Unlubricated version of CA-81. Highest Molecular weight.
Modulus of Elasticity 3.40 GPa
493 ksi
ASTM D638
Plaskolite West Optix® CA-81 General Purpose Acrylic Resin
Extrusion Grade Pellets. Highest Molecular weight.
Modulus of Elasticity 3.40 GPa
493 ksi
ASTM D638
Performance Polymers IPS II PPL-A1050 PEKK (Polyetherketoneketone) Branched Standard Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Modulus of Elasticity 3.40 - 12.0 GPa
493 - 1740 ksi
Average value: 6.02 GPa Grade Count:25
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Modulus of Elasticity 3.40 - 29.0 GPa

@Temperature -40.0 - 250 °C
493 - 4210 ksi

@Temperature -40.0 - 482 °F
Average value: 12.3 GPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Modulus of Elasticity 3.40 - 29.0 GPa

@Thickness 1.60 - 3.17 mm
493 - 4210 ksi

@Thickness 0.0630 - 0.125 in
Average value: 12.3 GPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Modulus of Elasticity 3.40 - 17.2 GPa
493 - 2500 ksi
Average value: 8.40 GPa Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
Modulus of Elasticity 3.40 - 17.0 GPa
493 - 2470 ksi
Average value: 8.25 GPa Grade Count:10
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Modulus of Elasticity 3.40 GPa
493 ksi
25mm flat samples, compression moulded; ISO 527-4
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP
SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi..
Modulus of Elasticity 3.40 GPa
493 ksi
ISO 527-2
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
Modulus of Elasticity 3.40 GPa
493 ksi
Conditioned; ISO 178
Addiplast Addinyl B2 V20 Nylon 6. 20% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Modulus of Elasticity 3.40 GPa
493 ksi
Conditioned; ISO 178
Addiplast Addinyl B2 ZV20 Nylon 6, 20% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Modulus of Elasticity 3.40 GPa
493 ksi
ISO 178
Addiplast Addilene J 220 M40 Polypropylene Copolymer
Mineral reinforced, improved rigidityInformation provided by Addiplast.
Modulus of Elasticity 3.40 - 11.0 GPa

@Temperature 120 - 200 °C
493 - 1600 ksi

@Temperature 248 - 392 °F
Average value: 5.89 GPa Grade Count:7
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Modulus of Elasticity 3.40 GPa
493 ksi
Conditioned; ISO 178
Addiplast Addinyl C2 V20 Nylon 66/6, 20% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Modulus of Elasticity 3.40 - 4.40 GPa
493 - 638 ksi
Average value: 4.07 GPa Grade Count:3
Overview of materials for PEKK, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate..
Modulus of Elasticity 3.40 GPa
493 ksi
ISO 527
BASF Ultramid® B3S BK00464 PA6 (Dry)
Ultramid B3S BK00464 is an easy flowing, pigmented black, finely crystalline injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Modulus of Elasticity 3.40 GPa
493 ksi
ISO 527
BASF Ultramid® B3S HP PA6 (Dry)
Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing
Modulus of Elasticity 3.40 GPa
493 ksi
Conditioned; ISO 178
Addiplast Addinyl C2 ZV20 Nylon 66/6, 20% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Copyright © lookpolymers.com All Rights Reserved