Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | STN 34 6460 |
Plastcom SLOVAMID® 6/66 FRC 3 TS PA6/66 flame retarded, heat stabilized PA 6 + PA 66 alloy for injection molding, reinforced with 30 % glass fiber, flame retarded with non halogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 5 a.. |
|||
Surface Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
Lehmann & Voss LUVOCOM® 1105-7238 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Surface Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
Lehmann & Voss LUVOCOM® 1105-7835 PEEK, with glass fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts,.. |
|||
Surface Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
Lehmann & Voss LUVOCOM® 1502-7866/GN4 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
Surface Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
Lehmann & Voss LUVOCOM® 1-7805 Polyamide 66, with glass fiber, aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Heat stabilised.High dimension.. |
|||
Surface Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
Lehmann & Voss LUVOCOM® 1-7904 VP Polyamide 66, unreinforced, thermally conductive modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Isotropic shrinkage characteristics.Reduced moment of inertia compared with.. |
|||
Surface Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
Lehmann & Voss LUVOCOM® 80-7666/GY Polyacetal-copolymer, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re.. |
|||
Surface Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
Lehmann & Voss LUVOCOM® 1105-8127-1 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Surface Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
Lehmann & Voss LUVOCOM® 1800-8504 PET, with glass fiber, thermally conductive modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Coil formers, duty parts in plugs and switches, even combined w.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, Conditioned Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Solvay TECHNYL® A 218 V35 Black 34 NG PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Solvay TECHNYL® A 216 NATURAL FA PA66, Conditioned Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | DIN 53482 |
Polyram PlusTek PA305G6 Nylon 6.6, 30% Glass Fiber Heat stabilized, improved surface quality, 30% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Polyram PlusTek PA804 Nylon 6.6 for Injection Molding, Impact Modified Impact modified Nylon 6.6 for injection molding application.Information provided by Polyram. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Polyram PlusTek PB300G4 Nylon 6 for Injection Molding, 20% Glass-Fiber Reinforced 20% Glass fiber reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | DIN 53482 |
Polyram PlusTek PB350M4 Nylon 6, 20% Mineral Filled 20% mineral filled polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® BG-25 HM PA6-GF25 Product description: Grilon BG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 25% glass fibers. Grilon BG-25 HM has the following important prop.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® BG-40 HM PA6-GF40 Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000/42 GV 15 HWCP 15% Glass Fiber Nylon 6, Polymer Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6600 GS 30 HWCP 30% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® L 20 GM PA12 Product Description: Grilamid L 20 GM is a medium viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics. Special features of.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® LV-3H PA12-GF30 Product description: Grilamid LV-3H is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® TR 30 LS nat PA* Product description: Grilamid TR 30 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 30 LS natural contains a processing a.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
DuPont Performance Polymers Crastin® FG6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6130 NC010 is an unreinforced medium high viscosity polyb.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
CENTROPLAST CENTROMID 12 soft Polyamide 12 soft This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | |
Radici Radilon® A CF350 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+14 ohm | 1.00e+12 - 1.00e+14 ohm | Average value: 8.08e+13 ohm Grade Count:13 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |