Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.990 - 2.26 g/cc | 0.0358 - 0.0816 lb/in³ | Average value: 1.28 g/cc Grade Count:31 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Density | 1.34 - 2.26 g/cc | 0.0484 - 0.0816 lb/in³ | Average value: 1.67 g/cc Grade Count:14 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |