Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Nilit FRIANYL B63 TF30 Nylon 6 for injection molding, 30% PTFE lubricated
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.34 g/cc
0.0484 lb/in³
±0.02 g/cm³; DIN 53479
PolyOne Bergamid™ A700 G20 U-SO Polyamide 66 (Nylon 66)
Information provided by PolyOne
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Celanese Vandar® 4632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Vandar 4632Z is a high impact, 15% glass reinforced polyester alloy. It combines high strength and toughness with a moderate degree of rigidity. It is characterized by excellent solvent resistance, ..
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
DSM Arnite® D00 301 PET (European Grade)  (discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced
Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Nilit RECONYL B KV30 Recycled nylon 6 for injection molding, 30% glass ball reinforced
Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183/A
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, DRY
Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr..
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP RFL32 PA 66
LNP* Lubricomp* RFL32 is a compound based on Nylon 66 containing 10% Glass Fiber, 15% PTFE. Added feature of this material includes: Wear Resistant.
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Techmer ES Elastoblend® PA6 GF34 IM HS 34% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 34% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac..
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
SABIC Innovative Plastics ULTEM PW2100 PEI (Europe-Africa-Middle East)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified...
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® 357 PBT
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region.
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Solvay Specialty Polymers Ryton® QA200N Polyphenylene Sulfide (PPS)
Ryton® QA200N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance.Features: Good Chemical Resistance; Good Thermal StabilityAdditional Pr..
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC
LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea..
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GB25 L BK 25% Glass Bead Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 25% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Density 1.34 - 1.40 g/cc
0.0484 - 0.0506 lb/in³
OSTM059
Solvay TOLCIDE® PS 70A 70% tetrakis hydroxymethyl phosphonium sulfate
Identification: CONCENTRATE BASED UPON TETRAKIS(HYDROXYMETHYL)PHOSPHONIUM SULPHATE (THPS) AND A BIOPENETRANTCAS: 55566-30-8Function: Concentrate for formulation into TOLCIDE® PS70A, PS50A & PS20A..
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
SABIC Innovative Plastics ULTEM 9085 PEI Blend (Europe-Africa-Middle East)
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 55/55 with low toxicity, smoke and flame evolution.
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East)
FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications.
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Plenco 7487 Phenolic, Granular, Transfer Molded
PLENCO 07487 is a rubber modified organic reinforced phenolic molding compound offering improved mechanical strength and lower modulus. Plenco 07487 is available in black.Information supplied by Ple..
Density 1.34 g/cc
0.0484 lb/in³
(DAM); ISO 1183
DSM Akulon® K222-KGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Covestro Makrolon® GF8001* Polycarbonate, 20% Glass Filled
ISO 7391-PC,MR,(,,)-18-3,GF20Developmental productFormerly Makrolon DP1-1951MVR (300 °C/1.2 kg) 16 cm3/10 min20 % Glass fiber reinforcedLow viscosityEasy releaseInjection molding - Melt temperature..
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Eurostar Starflam PX08029 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PX08029 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Covestro Makrolon® DP1-1888* Polycarbonate, 20% Glass Filled
ISO 7391-PC,MR,(,,)-09-3,GF20Developmental productMVR (300 °C/1.2 kg) 10 cm3/10 min20 % Glass fiber reinforcedMilled fiberMedium viscosityEasy releasegood surface qualityInjection molding - Melt te..
Density 1.34 g/cc
0.0484 lb/in³
Side 2, Silicone Property; Arlon SQA-TMS-024
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat..
Density 1.34 g/cc
0.0484 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 55580R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values for th..
Density 1.34 g/cc
0.0484 lb/in³
Layer 1, Silicone Property; Arlon SQA-TMS-024
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This..
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned)
Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability.
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Plaslok 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 302 is a two-stage, woodflour and flo..
Copyright © lookpolymers.com All Rights Reserved