Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 280 °C | 536 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Techtron® HPV PPS (ASTM Product Data Sheet) |
|||
Melting Point | 280 °C | 536 °F | |
Solvay Specialty Polymers Primef® 5084 30% GF PPS, Lubricated Grade
(discontinued **) Contains PTFE lubricant. Used for injection molding of high performance parts. |
|||
Melting Point | 280 - 282 °C | 536 - 540 °F | Average value: 281 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Melting Point | 280 - 285 °C | 536 - 545 °F | Average value: 281 °C Grade Count:23 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | DSC |
Solvay Specialty Polymers Hyflon® MFA® P6310 Perfluoropolymer Hyflon® MFA P6310 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti.. |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Melting Point | 280 °C | 536 °F | ISO 11357-3 |
Solvay Specialty Polymers Ryton® QC160N Polyphenylene Sulfide (PPS) Ryton® QC160N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Ch.. |
|||
Melting Point | 280 °C | 536 °F | ISO 11357-3 |
Solvay Specialty Polymers Ryton® QC160P Polyphenylene Sulfide (PPS) Ryton® QC160P (pelletized) polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Chemical Resista.. |
|||
Melting Point | 280 °C | 536 °F | GB/T 16582-2008 |
Sichuan Deyang Haton® hb DL Polyphenylene Sulfide Resin Extrusion, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melting Point | 280 °C | 536 °F | GB/T 16582-2008 |
Sichuan Deyang Haton® hc Polyphenylene Sulfide Resin Fiber gradeInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melting Point | 280 °C | 536 °F | GB/T 16582-2008 |
Sichuan Deyang Haton® hd Polyphenylene Sulfide Resin Film gradeInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melting Point | 280 °C | 536 °F | GBT/T 19466.3-2004 |
Sichuan Deyang Haton® hGR40 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melting Point | 280 °C | 536 °F | GBT/T 19466.3-2004 |
Sichuan Deyang Haton® hGR505 Polyphenylene Sulfide/PA Alloy Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melting Point | 280 °C | 536 °F | GBT/T 19466.3-2004 |
Sichuan Deyang Haton® hMR60DL Polyphenylene Sulfide, Glass & Mineral Reinforced Injection molding, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melting Point | 280 - 290 °C | 536 - 554 °F | |
A. Schulman ComAlloy Hiloy® 758 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has b.. |