Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Izod Impact, Notched (ISO) | 7.00 - 7.00 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.00 kJ/m² Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Crastin® SK603 BK851 PBT
(Unverified Data**) Crastin® SK603 BK851 is a 20% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Victrex® PEEK 450P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, standard flow, FDA food contact comp.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 7.00 kJ/m² @Temperature -40.0 - -40.0 °C |
3.33 - 3.33 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 13.1 kJ/m² Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | ISO 180/1A |
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Grupo Repol Dinalon® A1S25 G25PV0 25% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 66 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP PI001 PA 6 (Europe-Africa-Middle East) LNP* LUBRICOMP* PI001 is a compound based on PA 6 resin containing Silicone. Added features include Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP RFL36U PA 66 LNP* LUBRICOMP* RFL36U is a compound based on Nylon 66 resin containing 15% PTFE, 30% Glass Fiber. Added features of this grade include: Wear Resistant, UV Stabilized. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP UCL16AS PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, containing Carbon Fiber and PTFE. Added features include Heat Stabilized |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Lubricomp UCL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36AS is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.This data .. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP WFL34 PBT LNP LUBRICOMP* WFL34 is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS LNP* THERMOCOMP* AF003 is a compound based on ABS resin containing 15% Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES (Asia Pacific) LNP* Thermocomp* JF004EXP is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP UX05504 PPA (Asia Pacific) LNP* THERMOCOMP* UX05504 is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | ISO 180/1A |
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, DRY Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | 180/1A |
Total PS CPDS 827 Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) 827 is a high impact flame retardant polystyrene for use in HGW applications. PS CPDS 827 can be supplied in both natural and colored forms.Main Characteristics:DBD.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 BK851 is a 30% glass fiber reinforced black polybutylene terephthalate blend for injection mol.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -40.0 °C |
3.33 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | ISO 180/1A |
DuPont Performance Polymers Delrin® 527UV BK701 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV BK701 is a medium viscosity black acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has im.. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl C2 M20 V10 Nylon 66/6, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 7.00 kJ/m² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Izod Impact, Notched (ISO) | 7.00 - 15.0 kJ/m² | 3.33 - 7.14 ft-lb/in² | Average value: 12.5 kJ/m² Grade Count:11 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched (ISO) | 7.00 - 54.6 kJ/m² | 3.33 - 26.0 ft-lb/in² | Average value: 10.7 kJ/m² Grade Count:24 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 10.0 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 8.00 kJ/m² Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |