Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Mold Temperature = 350 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 65.6 - 177 °C
150 - 350 °F
Oxford Polymers PEI 30GF-Natural PEI, 30% Glass Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), Polyetherimide injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents Special Characteristic..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1305 TFE 15 Z Polyphenylene Sulfide (PPS), Glass Fiber - PTFE Lubricated - FDA Compliant Ingredients &a
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1300 C GB 40  Polyphenylene Sulfide (PPS) Glass Bead 40%  (discontinued **)&
Glass Bead 40%Comments:Glass BeadUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1307 C L  Polyphenylene Sulfide (PPS) Glass Fiber 40% - Lubricated  (discont
Glass Fiber 40% - LubricatedComments:Glass FiberLubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided b..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1381 TFE 15  Polyphenylene Sulfide (PPS) Carbon Fiber 10% - PTFE 15%  (disco
Carbon Fiber 10% - PTFE 15%Comments:Carbon FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provi..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2100 AR 15 TFE 10  Polyetherimide (PEI) Aramid Fiber 15% - PTFE 10%  (discon
Aramid Fiber 15% - PTFE 10%Comments:Aramid FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provi..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2100 HF SI 2  Polyetherimide (PEI) Silicone 2% - High Flow  (discontinued **
Silicone 2% - High FlowComments:Silicone LubricatedHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2100 Z  Polyetherimide (PEI) FDA Type  (discontinued **)
FDA TypeComments:FDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this ..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company EMI 2181  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 10%  (disc
Shielding - Nickel-Coated Carbon Fiber 10%Comments:EMI/RFI ShieldingESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pig..
Mold Temperature 130 - 177 °C
266 - 350 °F
Average value: 149 °C Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1300 D TFE 20 Polyphenylene Sulfide (PPS), PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1305 D TFE 15 Polyphenylene Sulfide (PPS), Glass Fiber - PTFE Lubricated - UL94 V-0
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1379 Polyphenylene Sulfide (PPS), Glass Fiber - Mineral
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1382 HEC Polyphenylene Sulfide (PPS), Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1385 TFE 10 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced - PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1389 HEC Polyphenylene Sulfide (PPS) Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI Shielding
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1487 N Polyethersulfone (PES), Carbon Fiber - High Viscosity
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1499 X 92453 Polyethersulfone (PES), Carbon Fiber
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2181 TFE 15 SI 2 Polyetherimide (PEI) Carbon Fiber - PTFE Lubricated - Silicone Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2184 L Polyetherimide (PEI) Carbon Fiber - Easy Molding
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1300 TFE 10 Polyphenylene Sulfide (PPS), PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1301 D Polyphenylene Sulfide (PPS), Glass Fiber
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1305 C Polyphenylene Sulfide (PPS), Glass Fiber
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1309 TFE 10 Polyphenylene Sulfide (PPS), Glass Fiber Reinforced - PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2100 LF TFE 10 Polyetherimide (PEI), PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2107 LF Polyetherimide (PEI), Glass Fiber - Low Flow
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2299 X 80218 Polyetheretherketone (PEEK), PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1402 N Z  Polyethersulfone (PES) Glass Fiber 15% - FDA Type - High Viscosity &nbs
Glass Fiber 15% - FDA Type - High ViscosityComments:Glass FiberFDA CompliantHigh ViscosityUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect p..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1399 X 91176 Polyphenylene Sulfide (PPS), Encapsulation Grade
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1303 Polyphenylene Sulfide (PPS), Glass Fiber - UL94 V-0
This series of compounds offer outstanding strengths combined with good heat and chemical resistance which may successfully be maintained in low load applications operating up to 500F. These ignitio..